Hi all!
I just found this chart in one of my dental text books. It contains info on the different types of dental gold available on the market and the gold, platinum, palladium content of each one. I think it's fairly up to date. I left off stuff like the hardness values but I can get it if anyone wants it.
I have it here as a spreadsheet. Hope this helps.
Tom
I just found this chart in one of my dental text books. It contains info on the different types of dental gold available on the market and the gold, platinum, palladium content of each one. I think it's fairly up to date. I left off stuff like the hardness values but I can get it if anyone wants it.
I have it here as a spreadsheet. Hope this helps.
Tom