C clwp Member Joined Nov 17, 2007 Messages 21 Location michigan Nov 25, 2007 #1 approx how many gold fingers will i need to process to make it worth while. I have approx 100 sitting around and was wondering what i could expect to recover from these. thank you
approx how many gold fingers will i need to process to make it worth while. I have approx 100 sitting around and was wondering what i could expect to recover from these. thank you
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Nov 25, 2007 #2 Not much unless they are high grade... You better wait to have a few pounds until you start processing them.
Not much unless they are high grade... You better wait to have a few pounds until you start processing them.