Process these whole or remove the fingers?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

skyline27

Well-known member
Joined
Jul 26, 2007
Messages
294
Location
Wisconsin
These dummy memory modules have many gold traces. Should I process these in AP as is, or should I remove the fingers like normal memory?
 
I had a similar question about Soundblaster live Sound cards

All the solder pads and logo and Ground plain have a gold foil over them I have a huge stack of them, most with components already removed. Is it cost effective to treat the whole card?

(Similar to these (large picture warning) http://mail.lipsia.de/~enigma/neu/pics/sb_live.jpg

I haven't really planned on processing electronic at all I'm just curious.
 
I would say for both the memory and the cards. Cut the fingers off and process the boards and the fingers separately. I am pretty sure that there will be other that will concur.
 
Thanks Jason. I use these parts to fix PC's for charity but some of them are useless like these so I've been hanging on to them. It's pilling up though Will have to junk(sell) it at some point
 