typical yield from 10 Intel 486 CPUs?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Exibar

Well-known member
Joined
Jan 18, 2008
Messages
80
Location
Mass
I searched and couldn't find the gold yield for 486 CPUs. What would th etypical yield be for 10 intel 486 CPUs? or if it's easier a pound of 486 CPUs?
I saw mention of a spreadsheet showing yields, but couldn't find it :-(

oh, hello all! This is my first post to a very needed forum! It's great to finally find a bunch of people that are interested in refining gold from electronics. I have to thank "no_reserve" on eBay for one of his auctions mentioning this forum :)

Mike B
 
cool, I have a bunch of them :)

Is there a spreadsheet or a listing somewhere showing the typical yield from different electronic parts?

thanks!
Mike B
 
The last time I processed a batch of 486 cpu's , I netted about 4.6 grams from 30 intel 486 dx2 . That would average out to about 4.50 apiece. Give or take at todays market price .
 