Some years ago i dismantled lots of relays and some had contacts containing >95% Pd, now i always thought these would been AgPd30 and AgPd60 but recently i read at doduco that their AgPd30 is just 30% Pd.
My question now is; AgPd30 / AgPd60 and such as AuNi5, are not molar mass formula? Does that mean AuNi5 contacts are actually 95% Au?
Also does anyone know the composition of "Gold F" contacts? (These are solid golden color, not flashed)
And.. are there AgPd contacts which are gold plated? I always thought they are just silver/copper base but im open for an correction now if any expert may
My question now is; AgPd30 / AgPd60 and such as AuNi5, are not molar mass formula? Does that mean AuNi5 contacts are actually 95% Au?
Also does anyone know the composition of "Gold F" contacts? (These are solid golden color, not flashed)
And.. are there AgPd contacts which are gold plated? I always thought they are just silver/copper base but im open for an correction now if any expert may