Identification (2) - Is there any PM in those chips ?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Uciocciu

Well-known member
Joined
Jul 30, 2018
Messages
53
hi guys,

take a look at those chips ?

do you think there is any PM to recover ?

Thank you in advance,
best

UCIOCCIUIMG_0910.JPG
IMG_0909.JPG
 
Hello,

I think my question sound slightly stupid (there is obviously some plated gold in the first picture :oops: ).

If by chance some of you have already dealt with these chips,
could you tell me wether OTHER precious metal are present ?

thank you in advance
Uciocciu
 
hello Uciocciu ,

that's nice to see the inside of the chips,
could you please tell me how could you remove the top part of the chips, really need help for these,

tks.
 
charlie2 said:
hello Uciocciu ,

that's nice to see the inside of the chips,
could you please tell me how could you remove the top part of the chips, really need help for these,

tks.

The ceramic layers are held together with glass. By heating them to about 700-800F and then quenching them in water, the glass with shatter and the layers will separate. Try this with one piece at a time until you find the right temperature. Try to not heat them hotter than necessary. I used an electric box furnace when I did them.
 