So I been processing some old what look like aux jax things that on first glance seem to be gold platted
So I started to strip them in a Sulfuric cell however the fizzing never stops and Amps don’t drop but the moment I rub them even ones half eaten away the Gold just re appears ????
So it it’s possible they could be made from a gold copper alloy? And if so what would be the best way to deal with them?
So I started to strip them in a Sulfuric cell however the fizzing never stops and Amps don’t drop but the moment I rub them even ones half eaten away the Gold just re appears ????
So it it’s possible they could be made from a gold copper alloy? And if so what would be the best way to deal with them?