Hello everyone,
I was shown this material today to consider a toll refining deal.
Since I barely work with silver-bearing scrap, I have some questions:
- Does the analysis seem legit?
- Is it worth to recover the silver, on a toll refining basis?
- I was thinking about using heated dilute nitric to dissolve the scrap and cement the silver out with copper. From my knowledge, either this or the chloride way, and I don't like the chloride way that much
Is there any other option?
Thanks in advance to anyone that can weigh in on this !!
Winged
I was shown this material today to consider a toll refining deal.
Since I barely work with silver-bearing scrap, I have some questions:
- Does the analysis seem legit?
- Is it worth to recover the silver, on a toll refining basis?
- I was thinking about using heated dilute nitric to dissolve the scrap and cement the silver out with copper. From my knowledge, either this or the chloride way, and I don't like the chloride way that much
Is there any other option?
Thanks in advance to anyone that can weigh in on this !!
Winged