dear masters

What can I get from the contactor parts shown in the pictures. I request your sublime information...
 

Attachments

  • IMG_20210506_170736.jpg
    IMG_20210506_170736.jpg
    3 MB · Views: 137
  • IMG_20210506_170748.jpg
    IMG_20210506_170748.jpg
    2.7 MB · Views: 137
Lacquered copper coils on an ferrous core. Laminated ferrous magnetic core pieces. Brass and copper contact parts with small contact points, probably containing silver and other metals.
Stainless steel pivot balls.

You could look up the data sheet if you can see partnumbers and manufacturer.

Martijn.
 
My advice will seem harsh but learn how to test for values and you won’t need to ask.
 