Limestone, feldspar, are the only abrasives in Bon Ami. it was once advertized as being gentle enough to be used as a tooth powder. I don't believe it has pumice. I'll let you know as I have a "lot" of silver scrap that I'll be parting this weekend. 8)
 
I think you're right. A lot of iffy sites say it does contain pumice. I had always heard it did. I found none that said it didn't. I did find 2 definitive-sounding sites that said those 3 ingredients on the MSDS were ALL it contained.
 