autumnwillow
Well-known member
- Joined
- Apr 1, 2010
- Messages
- 449
When a smelt is to be done instead of wet chemistry is it necessary to remove magnetics? If so, why? I know this is mentioned somewhere in Hoke's book, I've skimmed the book and have seem not to find it. This is after processing wastes. Whether sweeps, low grade, high grade etc.
The reason I ask is because I have forgotten the reason why I remove the magnetics. (After about a year of refining!)
I think some nickel white gold becomes a little bit magnetic when they are fine and are mixed with iron.
The reason I ask is because I have forgotten the reason why I remove the magnetics. (After about a year of refining!)
I think some nickel white gold becomes a little bit magnetic when they are fine and are mixed with iron.