In solution have white crystal

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

kuli

Member
Joined
Sep 25, 2017
Messages
12
Hello

Hello

I joined the forum because I have been dealing with gold for nearly a year and I'm always running out of the way.
When I add Urea and, finally, the SMB, at the bottom of the mud amateus, white ,, crystals ,,

Where do I break?
many thx
 

Attachments

  • CRISTAL 2.jpg
    CRISTAL 2.jpg
    3 MB · Views: 170
  • CRISTAL 1.jpg
    CRISTAL 1.jpg
    2.8 MB · Views: 170
In my experience,adding too much urea can cause this problems.

Sent from my ASUS_Z008D using Tapatalk
 
Hello

To much..But I put 1 tbsp. Can I solve the solution now or these is end?

regards
 
Yep looks like urea. The solution was probably left in a cold room.
After you do your water washes and hcl washes it will dissolve.
 
hi

Yes i left solution in cold room in celler. it a litlle bit cold.
Ok woudl you be so kind guys and tell me where in these forum i would like to found procedur how to wash solution?

Many thanks
 
Scroll down till you see the post by Harold V.
http://goldrefiningforum.com/phpBB3/viewtopic.php?f=49&t=325&hilit=pure+shiny#
 