Though I have never tried using a floc on a pregnant AR. I have successfully used PAC(Polyaluminum Chloride) after precipitation for about 1 out of 3 times. That one had no effect whatsoever on the gold output and the floc worked well, gold settled within 10 minutes, even during washing it settled fast. The other 2 attempts did not make gold settle at all but had no effect on the output product.
I wonder if I could use the same floc on a pregnant AR?
Ferric chloride is also used as a floc and I think its presence makes gold powder/silver chlorides settle better.
My theory is that with SMB sometimes the gold will settle fast and sometimes it doesn't. I think this is due to the presence of ferric chloride.
With copperas the result is usually consistent, maybe some of the iron converts into ferric chloride? Not sure though I'm no chemist.
I wonder if I could use the same floc on a pregnant AR?
Ferric chloride is also used as a floc and I think its presence makes gold powder/silver chlorides settle better.
My theory is that with SMB sometimes the gold will settle fast and sometimes it doesn't. I think this is due to the presence of ferric chloride.
With copperas the result is usually consistent, maybe some of the iron converts into ferric chloride? Not sure though I'm no chemist.