Hi all.
Some time ago I'm looking for the best way to roast sulphide ores leached and then extract the metal values contained therein.
To choose the method of roasting I have considered the material handling and performance you can get the resources I have.
After collecting a lot of information I found this way of roasting which I would like to share with you
I built the oven is circular fluidized bed which are beginning to publish data.
Theoretical considerations can be found at:
http://www.home.iitk.ac.in/ ~ bsreeni / cep.pdf
http://scialert.net/fulltext/?doi=jas.2011.1980.1986&org=11
Patent US4530169
Later I will give more details of the oven.
Some time ago I'm looking for the best way to roast sulphide ores leached and then extract the metal values contained therein.
To choose the method of roasting I have considered the material handling and performance you can get the resources I have.
After collecting a lot of information I found this way of roasting which I would like to share with you
I built the oven is circular fluidized bed which are beginning to publish data.
Theoretical considerations can be found at:
http://www.home.iitk.ac.in/ ~ bsreeni / cep.pdf
http://scialert.net/fulltext/?doi=jas.2011.1980.1986&org=11
Patent US4530169