It has been said by many that when you send a load to one of the small processors, that you aren't actually getting a realistic payment of what your boards actually had in them. That they cheat you out of whatever they can.
So, short of it being straight up fraud, because there was no umpire and they just cooked it in their favor...how do "they" steal the gold?
In another thread, Butcher describes how salt can cause gold to become more volatile at high temperatures by oxidizing it.
Along the way, from pyrolyzation to incineration to crushing etc....where are the "danger points"? Is it during the actual pyrolyzation / incineration?
So, short of it being straight up fraud, because there was no umpire and they just cooked it in their favor...how do "they" steal the gold?
In another thread, Butcher describes how salt can cause gold to become more volatile at high temperatures by oxidizing it.
Along the way, from pyrolyzation to incineration to crushing etc....where are the "danger points"? Is it during the actual pyrolyzation / incineration?