autumnwillow
Well-known member
- Joined
- Apr 1, 2010
- Messages
- 450
So I bought this high pressure burner and used an old aluminum pan, I put all these stone setter wastes in this aluminum pan, covered it and fired up the high pressure burner stove. As soon as smokes starts to appear, I light the smoke and it ignited resulting to no foul fumes at all.
After about 30 mins the smoke was no longer igniting, so I figured the pyro is almost complete. Well, I waited another 15 mins and noticed that the bottom of the aluminum pan is starting to melt. So I stopped, separated the gold from it and threw the aluminum pan.
Lesson learned, don't use aluminum pan for pyro.
I know about aluminum melting point being low, but I didn't know that a high pressure stove could actually reach that temp. What where they planning to cook on that kind of temp?
Anyway, so I bought this stainless pan. Upon looking at the box its actually a 3ply clad, stainless aluminum then stainless. It is how actually most stainless pans are manufactured for better heat distribution.
Definitely I don't think this stove can melt stainless, but what will happen to the aluminum that was sandwiched?
If it melts will it deform? Expand and explode?
After about 30 mins the smoke was no longer igniting, so I figured the pyro is almost complete. Well, I waited another 15 mins and noticed that the bottom of the aluminum pan is starting to melt. So I stopped, separated the gold from it and threw the aluminum pan.
Lesson learned, don't use aluminum pan for pyro.
I know about aluminum melting point being low, but I didn't know that a high pressure stove could actually reach that temp. What where they planning to cook on that kind of temp?
Anyway, so I bought this stainless pan. Upon looking at the box its actually a 3ply clad, stainless aluminum then stainless. It is how actually most stainless pans are manufactured for better heat distribution.
Definitely I don't think this stove can melt stainless, but what will happen to the aluminum that was sandwiched?
If it melts will it deform? Expand and explode?