I have a problem to determine copper in a magnesia cupel, at the end of the cupellation the cupel blackens, it has a dark colour so I can’t determine if the cupel has copper in it. Could it be that the problem is the cupel or the flux that I'm using? Please help If anyone has ever had this problem before.