Ceramic CPU's with PURE GOLD Bonding Wires!!!!

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

modtheworld44

Well-known member
Joined
Jul 13, 2012
Messages
407
Location
Chattanooga,TN
To All

Here is some pics of some Ceramic CPU's that,I have found to have gold bonding wires.Thank you patnor1011 for answering my question.


P.S There's about 8 pictures so please let me get the first two posts up.



modtheworld44
 

Attachments

  • DSC00279.JPG
    DSC00279.JPG
    4.5 MB · Views: 670
  • DSC00281.JPG
    DSC00281.JPG
    4.9 MB · Views: 670
  • DSC00282.JPG
    DSC00282.JPG
    4.9 MB · Views: 670
  • DSC00283.JPG
    DSC00283.JPG
    4.5 MB · Views: 670
  • DSC00284.JPG
    DSC00284.JPG
    4.7 MB · Views: 670
last pictures
 

Attachments

  • DSC00285.JPG
    DSC00285.JPG
    4.6 MB · Views: 667
  • DSC00286.JPG
    DSC00286.JPG
    4.4 MB · Views: 667
  • DSC00287.JPG
    DSC00287.JPG
    4.9 MB · Views: 667
  • DSC00288.JPG
    DSC00288.JPG
    4.6 MB · Views: 667
  • DSC00291.JPG
    DSC00291.JPG
    4.5 MB · Views: 667
From what I know of Patnor, English isn't his first language and I believe there may be a misunderstanding in terminology between you both. When I read bonding wires I mean the same things that Modtheworld just posted. I also believe that Patnor was referring to the wires from the pins through the ceramic to the point of what we would refer to as the bonding wires. I could be wrong so please feel free to tell me so.
 
Palladium said:
https://en.wikipedia.org/wiki/Wire_bonding

Palladium

Thank You for the link,I had not ever read that wiki page yet.It had some very good information on it.We're going to loose a lot of gold when all the company's finally end up using copper instead of gold.What will they do to us next,only time will tell.Thank You again for that great read.



modtheworld44
 
Mod, you will find this kind of wires in nearly all ceramic cpu's. Sometimes they are visible and sometimes they are inside black epoxy like substrate.
I said that there are no bonding wires in ceramic cpu - I meant ceramic itself, it is similar like with IC - bonding wires do not run the whole length from die to legs.
 