Hello I’m new to PM recovery etc. I’m trying to set up an indoor space in my detached garage-landfill. I tried one small experiment outside before but when I realized the gold quantity I got looked like Sreetips (YouTube and I believe Kadriver on here) dirty filter papers I decided to accumulate more to process and set up a indoor spot.
I saw some papers written on using silica gel or molecular sieves to absorb NO2 just wondering if anyone has tried it or not. Seems like a dry media to pass exhaust through would be ideal due to lower air pressure to pass through it.
I’m sure I read somewhere that the NO2 could be separated from the silica gel and the media reused.
Any thoughts?
I saw some papers written on using silica gel or molecular sieves to absorb NO2 just wondering if anyone has tried it or not. Seems like a dry media to pass exhaust through would be ideal due to lower air pressure to pass through it.
I’m sure I read somewhere that the NO2 could be separated from the silica gel and the media reused.
Any thoughts?