Ferrell
Well-known member
- Joined
- May 14, 2011
- Messages
- 83
We're wanting to purchase the formula/recipe for CLS by Action Mining, but we need to know how high the sulfur content is in our crushed ore. Do we need to send it somewhere to get it tested or is there a way we can find out how much sulfur there is in our ore? Thanks!