MonteDorado
Member
- Joined
- Jul 28, 2018
- Messages
- 9
So I have about 7 kilos of gold that is 85%+ purity. This gold has silver, platinum, rhodium, iridium, palladium, etc. I want to seperate the gold, purify it, and then precipitate the silver and pgms. I don't care about purifying the platinum, silver, etc. I just want the gold pure and the pgms and silver I can just ship out to the refinery. What would be the best way of going about this? I currently have oxalic acid 99.6%, sodium borohydride 98%, sodium metabisulfite 98.6%+, nitric acid 67.2%, sulfuric acid 98%, hydrochloric acid 32%, acetone 99.5%. Anything missing, let me know. I have plenty of lab glass and lab equipment. So, again, to summarize, I want pure gold, and to precipitate all else (any purity).
Thanks so much for all the help!
Sent from my BLA-A09 using Tapatalk