and i have looking for gold filled Jewelry and the price is not that high why is that.

what is this mean (solid yellow gold filled copper) is is fake gold

http://virginiemillefiori.com/blog/2015/04/15/3-things-you-should-know-about-gold-filled/
 
Gold filled or rolled gold is a solid gold plate or tube bonded to base metal or an alloy of base metals. It normally comes in 1/20 or 1/10 which means at least 5% or 10 % of the product should be karat gold.
Example 1/20 9 k weighing 20 grams should be 20 x 0.375 x 0.05 = 0.375 grams of fine gold.
1/20 14k weighing 20 grams should be 20 x 0.585 x 0.05 = 0.585 grams of fine gold.

Hope this helps.
 
nickvc said:
Gold filled or rolled gold is a solid gold plate or tube bonded to base metal or an alloy of base metals. It normally comes in 1/20 or 1/10 which means at least 5% or 10 % of the product should be karat gold.
Example 1/20 9 k weighing 20 grams should be 20 x 0.375 x 0.05 = 0.375 grams of fine gold.
1/20 14k weighing 20 grams should be 20 x 0.585 x 0.05 = 0.585 grams of fine gold.

Hope this helps.

it helps a lot..
but how can i see what is fake and what is real..
 
Denmark1970 said:
nickvc said:
Gold filled or rolled gold is a solid gold plate or tube bonded to base metal or an alloy of base metals. It normally comes in 1/20 or 1/10 which means at least 5% or 10 % of the product should be karat gold.
Example 1/20 9 k weighing 20 grams should be 20 x 0.375 x 0.05 = 0.375 grams of fine gold.
1/20 14k weighing 20 grams should be 20 x 0.585 x 0.05 = 0.585 grams of fine gold.

Hope this helps.

it helps a lot..
but how can i see what is fake and what is real.. but how can i refind it i read and read and see streetips videos from and am really sucks to MAT :(
 