A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,090 Location são paulo---brazil Sep 14, 2018 #1 i have stanous chloride----how many grams of it,i will need to dissolve in hcl to make a good testing solution? thanks in advance to all
i have stanous chloride----how many grams of it,i will need to dissolve in hcl to make a good testing solution? thanks in advance to all
J jimdoc Well-known member Joined Mar 12, 2007 Messages 4,945 Location Philadelphia Sep 14, 2018 #2 http://goldrefiningforum.com/phpBB3/viewtopic.php?f=48&t=2082&p=165528&hilit=stannous+jimdoc#p165528
A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,090 Location são paulo---brazil Sep 14, 2018 #3 thanks Jimdoc---it helped me Arthur kierski