temperature in a furnace for fusion of rh with nahso4

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

arthur kierski

Well-known member
Joined
Feb 10, 2008
Messages
1,090
Location
são paulo---brazil
i would like to know what temperature is used to fuse rhodium with sodiun bisulphate in a furnace?thanks in advance for yours answers´--------------------------------------------------------------------------------------------------------------------Arthur´
 
By trior and error,i found the temperature of 600 degrees centigrades for 3hours----it worked very well for me----and hope that will work for other members------thanks to all
 