I managed to get my cpu pins reduced to gold flakes. I kept them stored away for a year until I had the chance to get to use oxyathesetalyne to melt it at Its final stage....
The gold was pretty clean tho there was a tiny bit of green (copper maybe?) Residue. But very minimal.
I got the oxy on it for 10 mins or so and what I'm left with is a brittle black sponge substance which broke apart.
I've collected it all up but what's happened and where do I go from here??
Any help and advise would be much appreciated!!!
Thank you
I managed to get my cpu pins reduced to gold flakes. I kept them stored away for a year until I had the chance to get to use oxyathesetalyne to melt it at Its final stage....
The gold was pretty clean tho there was a tiny bit of green (copper maybe?) Residue. But very minimal.
I got the oxy on it for 10 mins or so and what I'm left with is a brittle black sponge substance which broke apart.