Hi
I had some problems in my first experience today.
1- I added slowly 1 liter nitric acid + 1 liter distilled water in some silver oxide batteries but after 2 minute acid fall out from erlenmeyer.
http://uupload.ir/files/oefs_bjklljhg.jpg
2- I see large volume of sludge in my solution. It covers my solution. Is this sludge normal ? ( I added some used filter papers to my solutions. Do they produce sludge?)
3- And major problem is NOx fumes. In videos in YouTube reactions complete in 20 or 30 minute. In my case I must add 2 liter acid to my batteries and I add 1 liter but after 8 hours I still see NOx fumes :shock: :shock: :shock:
Why ?
I add just 1 liter acid and some water and heat it. What is the problem ?
I had some problems in my first experience today.
1- I added slowly 1 liter nitric acid + 1 liter distilled water in some silver oxide batteries but after 2 minute acid fall out from erlenmeyer.
http://uupload.ir/files/oefs_bjklljhg.jpg
2- I see large volume of sludge in my solution. It covers my solution. Is this sludge normal ? ( I added some used filter papers to my solutions. Do they produce sludge?)
3- And major problem is NOx fumes. In videos in YouTube reactions complete in 20 or 30 minute. In my case I must add 2 liter acid to my batteries and I add 1 liter but after 8 hours I still see NOx fumes :shock: :shock: :shock:
Why ?
I add just 1 liter acid and some water and heat it. What is the problem ?