Hello,all.
At first,I want to say many thanks to you all.In this great forum,I can learn about recovery and refining precious metals.
Today I have a question about the way to separate silver chloride that mixed with tin chloride.
I have many silver chloride in my stock pot.unfotunately,they mixed with tin chloride.I don't know how to separate well.
I was try to dissolving the silver chloride with dilute hno3 but it didn't work.And then I try to convert mixed silver chloride to elemental silver using NaOh and sugar.
At this step,it look good.I get grey black cement like as elemental silver.But the silver is difficult to melt.the silver won't melt.They likely only ash.
What wrong with this?Anybody can help?
Thanks.
Sent from my ASUS_Z008D using Tapatalk
At first,I want to say many thanks to you all.In this great forum,I can learn about recovery and refining precious metals.
Today I have a question about the way to separate silver chloride that mixed with tin chloride.
I have many silver chloride in my stock pot.unfotunately,they mixed with tin chloride.I don't know how to separate well.
I was try to dissolving the silver chloride with dilute hno3 but it didn't work.And then I try to convert mixed silver chloride to elemental silver using NaOh and sugar.
At this step,it look good.I get grey black cement like as elemental silver.But the silver is difficult to melt.the silver won't melt.They likely only ash.
What wrong with this?Anybody can help?
Thanks.
Sent from my ASUS_Z008D using Tapatalk