Scrapper-aw-
Active member
- Joined
- Dec 12, 2009
- Messages
- 34
So in another thread I was talking about just learning about extracting Pt by itself. I keep attempting to drop with any batch that through assaying is known to have a decent enough percentage of Pt. If nothing else it's great practice and experience!
I have over a dozen filters with the precip from that many different attempts over the last couple of weeks sitting in a tub waiting to be incinerated. Yesterday we were working as usual with a couple different batches at once and one of them was on the heater having just had the Au sponge filtered off. We raise the temperature to 170*F to 180*F and then add our amonium chloride and, (in the past, but not with this particular batch), HCl.
Now, normaly we would also prepare an apx. 1 lb of amonium chloride with 500ml of water for each 8 liters of Pt - Pd laden liquid. We mix it into a slurrry and add it in that fashion.
With this batch we got it up to 189*F. When we added the amonium chloride laden liquid from the top of the slurry we san an INSTANT reaction. That was unusual. Immediately Pt started to drop out faster than I've ever seen it drop out. Since all the other Pt drops we've done have taken considerable time to complete we gave it about 90 minutes and filtered. This is what we captured on the filter!
http://dl.dropbox.com/u/3358180/Pt drop 12-15-09.jpg
For scale, this is a 22 cm filter paper. This should be about 1/4 to 1/2 oz. t. Pt. Our preliminary assay with our X-ray shows a purity of >93%! I will need to schedule some oven time in the near future. We've gotta have a cook off!!!
:lol:
I have over a dozen filters with the precip from that many different attempts over the last couple of weeks sitting in a tub waiting to be incinerated. Yesterday we were working as usual with a couple different batches at once and one of them was on the heater having just had the Au sponge filtered off. We raise the temperature to 170*F to 180*F and then add our amonium chloride and, (in the past, but not with this particular batch), HCl.
Now, normaly we would also prepare an apx. 1 lb of amonium chloride with 500ml of water for each 8 liters of Pt - Pd laden liquid. We mix it into a slurrry and add it in that fashion.
With this batch we got it up to 189*F. When we added the amonium chloride laden liquid from the top of the slurry we san an INSTANT reaction. That was unusual. Immediately Pt started to drop out faster than I've ever seen it drop out. Since all the other Pt drops we've done have taken considerable time to complete we gave it about 90 minutes and filtered. This is what we captured on the filter!
http://dl.dropbox.com/u/3358180/Pt drop 12-15-09.jpg
For scale, this is a 22 cm filter paper. This should be about 1/4 to 1/2 oz. t. Pt. Our preliminary assay with our X-ray shows a purity of >93%! I will need to schedule some oven time in the near future. We've gotta have a cook off!!!
:lol: