I hate to that guy but isn't 250 ml plus 110 ml equal 360 ml? The title says 250 ml.

Any way Thanks for another good video.

I should have watched the end before typing, :oops:
 
Ten ounces a liter is usually a pretty saturated solution, but you can go more.

Heck, you can have 600+ g/L platinum :)
 
It takes a little bit less than 0.3ml of nitric acid and 0.9ml of HCl to dissolve a gram of high purity gold.
 
autumnwillow said:
It takes a little bit less than 0.3ml of nitric acid and 0.9ml of HCl to dissolve a gram of high purity gold.

True. I've not run the exact maths however I've banged on for years on that 1ml of Nitric is not required per gramme of gold.
 
Since this video was posted I just assumed he generated chlorine gas then bubbled it through his HCl to dissolve sponge.