Greetings. I've had some good luck with A/P and pins not completely plated with gold, and of course gold fingers. I am running into an issue though with the gold plated pins. I don't really feel comfortable with Nitric and AR (I need to study more).
Does anyone have suggestions on how to get the gold off the completely plated pins I have? AP would take forever since the base metals aren't coming in contact with the AP. Am I stuck with Nitric, or is there another way to do this?
Thanks!
Viro
Does anyone have suggestions on how to get the gold off the completely plated pins I have? AP would take forever since the base metals aren't coming in contact with the AP. Am I stuck with Nitric, or is there another way to do this?
Thanks!
Viro