hello anyone
i have a problem with my gold...
i have 100 gold bars and i wnat refind but how can i get the other metals out of the gold bars
i have try with Aqua regia and that was total messed up and i only get a gray looking mud or glay
and i try to refin again but the color was getting green and was stille lot acid in it and yes i use urea
what can i do to get the metals out
i have a problem with my gold...
i have 100 gold bars and i wnat refind but how can i get the other metals out of the gold bars
i have try with Aqua regia and that was total messed up and i only get a gray looking mud or glay
and i try to refin again but the color was getting green and was stille lot acid in it and yes i use urea
what can i do to get the metals out