COOPdawg007$$
New member
- Joined
- Mar 8, 2017
- Messages
- 2
Hello my name is David, I have 2lbs of gold leaf, and the bottles say 22kt gold on them. I took to a very reputable jewelry store they told me it was gold but wanted to take all of it in their lab to test it all, I said no.... I then took to a pawn shop they put it in a machine, and told me it wasn't gold but had other metals in it, I want to process the gold out of it and smelt down into round coins or bars, but never done anything like this befors. I have hydrochloric acid bleach peroxide, and sodium nitrate, but what should I do first? To extract the gold? Please help me if you can