archeonist
Well-known member
- Joined
- Jun 27, 2012
- Messages
- 286
Hi guys, I'm looking to buy a gold test kit on the internet but I find them a bit expensive. Now I am thinking of making such a kit myself for nearly zero dollars.
I tried to find information about this topic but I only found a recipe for making Swerters solution.
I would like to know if there is a known recipe for testing 8, 14, 18, 20K gold. My guess is that it is just AR in various concentrations? Somebody who can help me with this?
I tried to find information about this topic but I only found a recipe for making Swerters solution.
I would like to know if there is a known recipe for testing 8, 14, 18, 20K gold. My guess is that it is just AR in various concentrations? Somebody who can help me with this?