Nauticamark
Member
- Joined
- Jan 25, 2015
- Messages
- 20
Hey all! So I have been refining my polishing sweeps per Harold_V's directions on "Recovering precious metals from polishing sweeps." So far, going good, and huge thank you to Harold_V for sharing that valuable knowledge. So my question is, has anyone tried to not use the AR process, and try the HCL-CL process? My thought on this was that the gold particulates are super fine, and from board discussions, the HCL-CL process is good for using on super fine material. Should I expect to have any particular issues or problems if I give this a shot, for the final process of extracting the gold?
Any feedback would be greatly appreciated!