Double refined took to refiner assayed at .9999 best I have done to date.
 

Attachments

  • IMG_1530.JPG
    IMG_1530.JPG
    1.2 MB · Views: 609
  • IMG_1535.JPG
    IMG_1535.JPG
    1.7 MB · Views: 609
One day I am going to try making a bar. I hope it looks as good as yours! Very Nice!
 
Thank you everybody for the compliments it means a lot coming from the experts! To all future refiners read study and study some more believe me it pays $$ off
 
That is the dimple that forms when gold of a high purity cools quickly. If you cool it slower by heating with a torch you can get concentric circles. I have heard that dimple called many things over the years, both here and in the refineries I visit, but there is no "official" name for it as far as I know.

Maybe now that we have over 40,000 members the GRF has the clout to pick a name and stick with it and the rest of the refining world can follow along.
 
Looks beautiful, if you feel like donating it to the uk I would gladly accept it!!! What weight is it?

Sent from my EVA-L09 using Tapatalk
 