:Gphilddreamer said:One never gets tired of contemplating gold... 8)
Phil
wow nice buttons..... wish I knew what to do with my growing collection of bits and crumbs ... for now looking at them makes me think I've what You have " PhDRMR " but I know theres work to do first... .. ( Suggestions are very Welcome )philddreamer said:Thank you all!
It's gold recovered from military/aerospace pins...
I like to melt them and run them thru P.AR ... the acids attack the base metals more readily. I run them thru AR for final refining.
That's the second batch; and more still to come in the next few months!