autumnwillow
Well-known member
- Joined
- Apr 1, 2010
- Messages
- 449
Small scale miners goldMGH said:Very nice looking gold. Even the flux on it is clean What was the source material? I'm guessing not e-scrap if you refined that much gold in a 4L vessel.
I did. It was hard to remove the purple flux. I ended up wiping it off multiple times with soap and sponge.anachronism said:It looks really nice. Pop it in some warm dilute H2SO4 and get rid of that borax and it'll look even nicer. 8)
autumnwillow said:I did. It was hard to remove the purple flux. I ended up wiping it off multiple times with soap and sponge.