patnor1011
Well-known member
While it has not much with refining as it is it involve precious metals precisely silver.
Anywhere you look colloidal silver is being sold for extremely over inflated prices yet it is so easy to make. I have no clue what warrant charging 20$ for 100-200ml yet that is about average price of what it is being sold.
I will not go in detail about what it can be used for, internet is full of information.
I did not wanted to focus on hard to prove but evident medical benefits and I am not trying to push it as a cure-for-all ailments but I wanted to focus rather on proved and tested antibacterial, antiviral and anti-fungal properties. There is no secret that silver is being used more and more often in hospitals and that got my attention.
This is work in progress and I am testing it for last few weeks and it seems as a good idea to make more out of your silver.
If anyone want to try this I can go into more details but for now here is what I do make and what I do have now.
Cost of making it? You need to invest little bit on start but after that it is pretty much negligent.
Anywhere you look colloidal silver is being sold for extremely over inflated prices yet it is so easy to make. I have no clue what warrant charging 20$ for 100-200ml yet that is about average price of what it is being sold.
I will not go in detail about what it can be used for, internet is full of information.
I did not wanted to focus on hard to prove but evident medical benefits and I am not trying to push it as a cure-for-all ailments but I wanted to focus rather on proved and tested antibacterial, antiviral and anti-fungal properties. There is no secret that silver is being used more and more often in hospitals and that got my attention.
This is work in progress and I am testing it for last few weeks and it seems as a good idea to make more out of your silver.
If anyone want to try this I can go into more details but for now here is what I do make and what I do have now.
Cost of making it? You need to invest little bit on start but after that it is pretty much negligent.