Hey guys,
Semi-longtime lurker of the GRF. I have some gold for sale that has been refined from fingers off of various PCI boards and Memory sticks.
I am unable to melt it to a button due to not owning a good torch. To achieve higher purity, I have dissolved the gold twice using AR. The gold was washed before and after the second dissolving with 3 cycles of HCL and 3 Cycles of Distilled water.
3.6g PM me.
Thanks
-Stefan