I got screwed by 2 different refineries

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
A

Anonymous

Guest
Arch Enterprises is the worst refinery I have ever dealt with. I "locked" in a price over the phone prior to sending in my gold. Then they apparently unlocked the deal since they sent me a check for about 30% less than I had locked in. They are total rip off artists.

I also had a problem with Midwest Refinery. They charged me a fee despite the fact that their website says they do not charge fees.

Now I send all my gold to the only refinery that never really screwed me, Kitco. I have been happy with them paying me 94%. I would rather deal with an honest company at 94%, than deal with empty promises of 98% or more.
 
I sent 8 ounces of pgm bearing Dore to Arch Enterprises. They told me they could not dissolve the bar in their AR pressure vessel and then refused to take calls from me. After being put on hold every time and then have the line just go dead I finally got the point. I do not know why so very many refiners would rather rip you off once than receive a regular flow of materials.

Randy in Gunnison
 
I second that question! Why let these people rip off your hard work, instead fight back. If you started the process over the internet, my son works with the FBI looking at internet fraud. If you sent them the materials via parcel post then there is mail fraud. Place a claim with Fedx or UPS for your loss. GET PRO ACTIVE! Get mad as hell and your not going to take it anymore. Look at all the federal commisions talk to them. Don't just accept the loss and move along. Fight back become a thorn in their side. IE a pain in the ASS!

Ray
 
and even better yet lets start a thread here with a good and bad expierences from various refiners. this will help the good guys get more product coming in and maybe make the scam artists (big or small) maybe take a hit in their pocket as well.
 
Once many years ago I was responsible for shutting down a car dealership that was ripping of their customers. I lived 8 miles from the dealership. The action, involving the California State Attorney General and the Better Business Bureau, took months. And it took a lot out of me.

Two years ago I shipped 8 pounds of fine gold powder to a west coast refiner by UPS. The gold was sealed in a special chemical shipment unit.
The package was insured. When it got where it was going the package was torn apart, the chemical shipment container was smashed, and the gold was gone. But because the receiving company accepted the package as is UPS would not honor an insurance claim. I don't ship anything by UPS, period.

If I was younger I would after some of these companies. But now I am 60 and have all kinds of health problems that relate to be a radiation down winder. So I pass it to others to go after the dirty boys (and they are everywhere). But if you need some insights on how to do it -- I've shut down companies and I've shut down a major drug network by working with the FBI (by major I mean 100 tons of cocaine a year).

Randy in Gunnison
 
Gentlemen (and ladies,too)

I am in complete agreement on starting a thread for refinery feedback and validation. That said, please refer to a new topic in this category, titled "Refineries- The Good, The Bad, and The Ugly".

I am going to also PM a few key players on this Forum to prompt their input. We all should share this information, for the good of all concerned.

Sincerely,

John
The Refiner49er
 
The only way to ship bullion or other hi-value PM material is USPS, Registered, Insured.

I think the terms Respectable Refiner, Honest Refiner, Honest Lawyer, Honest Politician, and Benevolent Banker are all oxymorons. There are exceptions, of course, but no one knows who they are. Also, things change with new managers.

I was once interviewed by several agents of the California Board of Corporations (or, whatever it's called) concerning the MO of refiners. After 2 or 3 hours, they decided there was no way to control it, since no one could prove what they had. About the only way to nail them is to set up a sting, with good professional assays and documentation.
 
i spent 25 years in the trucking ind before getting hurt, if you ship your materials by truck to a refiner, if they lose it ,can't do anything with it
and won't ship it back to you, contact the FBI. if you materials leave the
state,it becomes interstate theft.provide them with the bill of lading and
the pro# (fedex and the usps call them tracking #s) if your materials
stay in your on state call your state police or state investigaters.
when you ship by truck.unlike fedex or usps someone at the
refinery has to sign for it. stay proactive don't let anyone steal
from you

renegade
 
US Gold Buyers is by far the biggest crooks I've experienced. I hand delivered 65 toz of 14-k and was told they would have to do a melt to determine what I would recieve. They said they only charged 2%. Four hours later I recieved 8000. Less then I had caculated. They said over 16 toz was fake. I asked for the fake gold back and was told it was a already diposed of. Watch out for these crooks.
 
I hear a lot of complaints about being ripped off by refiners but it seems that few people know how to prevent it. How many of you would go into a bank with a pile of money and tell the teller that you don't know how much is here but if they will count it and credit your account you would appreciate it. You know sooner or later you'll get ripped off. Going to a refiner and handing them a pile of scrap to pay you for is the exact same thing. If you don't have the capabilities to melt the material go to the refinery and witness the melt, don't let it leave your sight. If the melt was large enough they will take a dip sample, make sure the melt is molten and stirred before sampling. If it is a smaller melt, still make sure it is molten and stirred before they pour it. Inspect the bar and the slag after the pour. If the slag has alot of beads put it in a bag and take it, it contains your metal. Now they will either drill your bar, make sure if it is a drilling they take it from both the top and bottom, if they took a dip sample they will cut it into small pieces. Both the cutting of the dip sample and the drilling will be done in front of you. They will package up 3 small samples of at least 1 1/2 grams each (1 pennyweight) I would request more sample, at least 3 grams so you have extra in case you need to run another assay. You take 1 sample, they keep 1 sample, and a 3rd is for an independent assayer in case you don't agree with their assay. I like to request the right to take my bar back if we don't agree on assay, so since all bars tend to look alike, sign the bar on both sides with a marking pen. Also sign the seal of the umpire sample. If you follow these steps they will know you have been around the block before and your settlement will be treated with respect. Now before you leave take a receipt with you which states the weight they will be paying you for. It should be the weight of the bar plus the weight of their sample, plus the weight of the umpire sample. Now it's just like you counted the money before going into the bank and you have a receipt. You now have recourse if you don't like the result!..Of course you have a written list of what the charges will be for the refining services, what metals they will be paying for (don't let them keep your silver either) And you had it before you went to the refiner in the first place. To be fair to the refiner, because there are refiners who do legitimate business and are entitled to make a reasonable profit, you will be paid a percentage of all metals refined and if some metals do not reach a minimum deduction you will not be paid for them. There are also things like splitting limits which means if your assay differs from their assay by more than a defined percentage (never over 0.25%) you will use the umpire sample to determine who is right. If you are within the splitting limits you split the difference. Umpire assays are not cheap and the looser pays the tab. Shop a few refiners, read their terms and do what I wrote above and you should be OK for melt-able scrap. Find a decent assayer and have your sample assayed, in the event of a difference, keep track of who wins, if your assayer looses too often, find another. A good assayer is like a good heart doctor except they don't make as much money.

If you follow the procedure above you will leave the refiner with no cash in hand, but you will have receipts which are legal documents. Send out your assay sample ASAP and when you have a result call the refiner to exchange assays. In most cases they will tell you their assays first, if their number is higher accept it and go to the next metal. This process will take a few days longer if PGM's are in the bar but you can usually settle gold and silver within 2 days. When you settle you tell them which day you want them to price your metal and they will cut a check for you on that day.

There are similar precautions for non melt-able scrap and if anyone is interested just ask. It isn't fair to complain about being ripped off if you didn't go into the refinery prepared.
 
4metals,

That was an excellent description, I learned from it, and I’m sure others will as well.

By all means post your standard operating procedure for non melt-able scrap.
 
From my previous post about melt-able scrap, you can easily figure out its all about the sample. If the sample is good it is representative of the entire lot. Melting is one of the easier samples to get representative quickly, other materials may require you be present as a representative of your material for 2 or 3 continuous work days. If you're not willing to do that, you have no gripe about low yields.

Some materials are sample-able as a fine 60 to 80 mesh powder, others are chopped or ground to make a homogenous mixture, often to prepare this material takes a few, time consuming steps. I am assuming that you have quantity of these materials because this process is never done for 25 pounds, there are small collector refiners who process small lots and the rules to follow are similar.

First lets talk about seals, not the furry kind that eat fish but the ones that make your drums and containers tamper proof. When you ship your material to a refiner, or take it in yourself always ship it in drums (usually 55 gallon size) that have open tops and lids with rings to seal them. Through the tabs on these drums you will place a numbered seal. These seals are your way of knowing nobody was in your drums without you being there to see them. Don't worry about hurting anybody's feelings refiners use them when they ship material out as well. Often incinerators or ovens are used to process your materials overnight, always put a seal on the door so it can't be opened until you are there the next day. Bring extra seals so you can close up drums of processed materials that you can't be with. While we're on the subject of drums, often a large refiner will provide you with drums for shipping, I always accept. If they offer you seals, always decline. Don't cheap out here, buy seals which are numbered and colored various colors so they cannot be duplicated easily.
Write down what the drums weigh empty, full, and net weight of your material and write down your seal number. This is necessary documentation for the refiner to receive your material.

Tell the refiner what you are bringing and discuss how it will be sampled and the time required. Also discuss rates before you arrive and have them in writing. This is always done by appointment, you don't just drop in.

If your material is a fine mesh powder, usually called prepared sweeps, the process you will witness is called blending, whereby all of the drums of powder are mechanically added to either a double cone or a vee blender and blended for 45 minutes. The powder is then returned to the drums and each drum is sampled with a pole sampler made to sample the powder evenly all the way down to the bottom of the drum. The technical name for the sampling pole is a thief. Kind of ironic but they come from the grain industry and they call them grain thiefs. (just a little historical perspective) Now all the drums are sealed up with the refiners seals and weighed to get your final weight. You're done with the drums now focus all of your attention on the sample pulled from the drums. Some refiners will weigh out 500 grams of sample, often in duplicate, and place it in an oven overnight to calculate the moisture content. Make sure you seal the oven. This material can be as rich as 1 ounce of gold per pound, so a 2000 pound lot (4 drums) can be 1/4% moisture and it represents real money. The moisture is calculated in the morning from the samples dried overnight and the weight of water in your entire lot is subtracted from the totals. Now bags of sample are prepared for you to take for analysis. Always take at least 1 ounce, they take an ounce and again an umpire sample is sealed up as well. Now you're done, you have weights and a representative sample and your seals helped you verify nobody messed with your samples.

Next post we'll discuss preparing sweeps at a refiner, here are a few pictures of what seals look like.
 
Burning crushing and sifting. Sampling material that needs incineration and sweeps preparation is never a 1 day deal. When your drums arrive at the refiner, with your seals on them, they will call you to schedule your visit. Always let them know when you intend to come or would like to come and schedule delivery so the material isn't at the refinery too long. Who knows what can happen, you've safeguarded the scrap this long so be safe. They will put the material into the incinerator and start a burn cycle. If they say it will need raking during the process be there when the oven is opened. Usually they burn overnight so seal up the oven until the morning. Your material is ready for crushing in the morning, usually after a rake to see if it's still smoldering, if it is let it burn out. Before the material is put into a ball mill, check to see that there are only balls in the mill. Have them install the dump grate and spin the mill to make sure no left over material is in the mill. Add your material to the mill and let it crush for the required time, usually 1 hour. They will then dump the mill into the enclosed housing and take your crushed powder to the sifter. Again have them spin the mill to assure it is empty. Some representatives make the refiner weigh the material out of the incinerator so they can track the weight and be sure it is all there after milling and sifting. (Not a bad policy) Finally the material is sifted, the majority of the fine powder represents your greatest values, this is where your samples will come from using the sampler the same as in the previous post. They rarely dry a sample after incineration because it hasn't had time to pick up moisture. There is oversized material in the sifter, it is your material and it almost always contains values. Have it put in a 5 gallon pail and put a seal on it and take it home. When you accumulate enough of this stuff bring it back for crushing and sifting again. Usually there are 3 fractions coming off the sifter, the oversize is broken down into magnetics (low value) metallics (higher value, usually there's bigger pieces of gold in there) and chunks of wanna be powder that didn't crush. You want it all. If there's a large fraction of metallics the refiner may suggest melting it. Finish with your sweeps samples and rep the melt just like the method described for melt-able scrap.

Again you will leave with paperwork stating the settlement weight, you will have sealed up an umpire sample and you have your sample. And you have seen it all processed before your eyes.

The last type of material to watch at a refiner is e-scrap, my next post will detail that sampling process, I have to rest my fingers.
 
The last and possibly the most popular type of scrap (for this forum) to send out to a refiner is e-scrap. From what I've read on this forum a-lot of our members get this scrap and cherry pick the good stuff for refining or do some sort of preparation so they can recover the metals from the higher yield components themselves. This will always leave some kind of lower yield material that is ripe for sending out, providing you can get paid fairly for what's in there. Again the only way to tell what is in there is to sample the material and the sample has to be representative. This material is generally stream sampled. What that means is they chop, shred, grind or pulverize the material into uniform sized chunks so they can draw off a proportional sized sample. A stream sampler will sample shredded paper as well as it will sample lead shot, and therein lies its weakness. It is up to you, the generator of the material, to separate the material into grades of like density scrap. This is a bit of subjective sorting here but let me explain. The material which has been processed into like sized pieces is moved along a conveyor and dropped into a chute as a steady stream of parts, the machine is programmed for say a 25% sample, by switching some diverting arms the sample streaming down the chute is diverted into different lines, one line goes to the 75% accumulating pile, and the other to the 25% pile. It is amazing to watch and I have watched it and weighed the fractions coming off and it's pretty dang close to right on. This procedure will then be repeated on the 25% fraction to produce a fraction which is 6 1/4% of the original and so on. They continue until you have a representative, manageable sample of the entire lot. This sample is either incinerated, crushed, sifted, and the oversize melted with copper, or it's melted directly with copper. The benefit is the smaller sample is produced into an assayable sample while you watch.

Now for the glitch...... :twisted: ........if the material is a mixture of say steel relay headers with gold pins, and depopulated PC boards, the sampling will not be so great. The heavier steel headers fall faster than the light circuits so the stream isn't as dense consistently. Now if you have enough headers to run separately, and enough boards to run separately, the densities will be similar and the sampling is very good. The refiner doesn't know if a bad density mix will work in his favor or in your favor so he isn't too anxious for sampling of poorly sorted materials either. So the sorting is the job of the collector, you, before you ship for stream sampling.

The material which you have pre sorted is received at the refiner where they will decide if it will be best to granulate, shred, ball or hammermill this material before stream sampling. Whatever they decide, you will be part of the decision, and with your nod the material will go through the tortuous process. You will know your start weight and verify the finish weight. From looking at the parts they will also let you know if it will need incineration (likely if it was PC boards) or straight melting. Now it's off to the stream sampling machine. I've brought in 20, 55 gallon drums of plated connector scrap and had it reduced to 3, 5 gallon pails. Now you get to do eenie meeney miney mo and pick one for processing. The other two are sealed up in case another sample is needed.

If the material has to be incinerated, you will end up with a powdered sweep portion which is sampled for assay just as described for sweeps processing, the only difference is the rather large metallics fraction. Actually they mix magnetics and metallics together for a melt with copper.
You will witness the melt and just as before with meltables come away with samples and a sealed umpire. If the job didn't have to be incinerated, it goes directly to the melt room.

In both cases you have come away with samples which you witnessed and are reasonably sure represent your material.

This last type of processing is only done by rather large refiners and if they will not let you witness everything, say thank you and find another refiner who will. If you do enough of this type of recovery, and keep records about different materials you will generate enough data to feel confident that you are getting your just return. Just don't get confident enough to let them process it without you there.

There are others on this forum who have witnessed materials as I have and I invite all comments concerning what I have said or more importantly about what I may have missed.
 
Once others have given their input this should be made into a tutorial or sticky post.
 