tensecondsdown
New member
- Joined
- Apr 14, 2018
- Messages
- 3
Hi, I refined some gold by inquartation and that worked fine. I put a copper plate in the silver nitrate to cement the silver out. I think there was still some nitric acid in it but I read that it would not matter as it would just re dissolve the silver until it was used up then cement out fully. I rinsed the powder a bunch of times and dried it and the powder has a blue tinge to it so I don't thin I got all the copper out. Should I just rinse it some more or is there something I can use to dissolve just the copper? Thanks.