Processing fingers in poor man's nitric acid

Post by Geo » June 12th, 2018, 2:53 am

This is my video on making and using poor man's nitric acid. I can't get the video to embed so you will have to follow the link.

https://youtu.be/-Lojvw46Kgk
"knowledge is power"
https://www.facebook.com/groups/1778525 ... oup_header
E-WASTE AND PRECIOUS METAL REFINING

junkandtreasure
Member
Posts: 2
Joined: August 24th, 2014, 11:01 am
Country of Origin: USA
Location: Florida Panhandle

Re: Processing fingers in poor man's nitric acid

Post by junkandtreasure » June 14th, 2018, 7:48 am

Thanks Geo, a very informative video.
I noticed a couple of comments regarding a white powder residue.
I have a bag of the Hi-Yield Nitrate of Soda and there is a note
on the label that it contains 580 lbs of Calcium Carbonate CaCO3
per ton (%29).
I'm not a chemistry whiz, but I think some insoluble compound is
being produced from it reacting with either the H2SO4 or the HNO3
produced.
Perhaps some member could provide more information on the
chemistry involved.

User avatar
g_axelsson
Active Member
Posts: 4736
Joined: November 17th, 2007, 8:46 pm
Location: Sweden

Re: Processing fingers in poor man's nitric acid

Post by g_axelsson » June 14th, 2018, 2:39 pm

Calcium sulfate would precipitate as a white powder... it's gypsum.

Göran
Visit the GoldRefiningWiki, an online refining encyclopedia.
It also contains an online version of the book "Refining Precious Metal Wastes" by Hoke.

User avatar
Geo
Active Member
Posts: 6423
Joined: March 1st, 2011, 7:56 pm
Country of Origin: U.S.A.
Location: Decatur,Ala.

Re: Processing fingers in poor man's nitric acid

Post by Geo » June 14th, 2018, 10:02 pm

Thanks junkandtreasure. I will have find out if that is the same brand wide or regionally. I may have to buy a better grade.
"knowledge is power"
https://www.facebook.com/groups/1778525 ... oup_header
E-WASTE AND PRECIOUS METAL REFINING

kurtak
Active Member
Posts: 1707
Joined: January 16th, 2014, 12:37 pm
Country of Origin: USA
Location: Central Wisconsin

Re: Processing fingers in poor man's nitric acid

Post by kurtak » June 16th, 2018, 11:27 am

Geo wrote:Thanks junkandtreasure. I will have find out if that is the same brand wide or regionally. I may have to buy a better grade.
Geo

Have you considered using "Spectracide" brand stump remover as your nitrate source - it is potassium nitrate which I believe does not have any other additives such as the Calcium Carbonate in the Hi-Yield (its straight up potassium nitrate)

I have never had to make poor mans nitric because I have always had access to cheap nitric - I however do use the Spectracide (potassium nitrate) as a flux ingredient in "some" of my smelting flux's when I think I need an added oxidizer in the flux (its hard on crucibles so only use it if/when I think I need the added oxidizer)

The Hi-Yield (I believe) has the Calcium Carbonate (a base) in it to act as an inhibiter so that the nitrate is time released as a fertilizer - other wise the nitrate would release/dissolve to quickly & burn the plants you are fertilizing with it

Spectracide stump remover can be found in the garden department of Home Depot or Lowes &/or most other farm & garden shops

As an added note; - you have to peel the label on the back of the Spectracide bottle to see that it's potassium nitrate

Kurt
You do not have the required permissions to view the files attached to this post.

User avatar
denim
Active Member
Posts: 251
Joined: March 13th, 2012, 10:15 pm
Country of Origin: usa

Re: Processing fingers in poor man's nitric acid

Post by denim » June 16th, 2018, 2:20 pm

Hey Geo,

I know that 'watching the bottom line' is paramount in our small scale refining world, but why not just buy some sodium nitrate from Duda Diesel which is 99% pure, and cheap- $12.50 for 5 lbs plus some shipping. I buy mine this way and 5 lbs lasts me a couple of years. I don't do fingers in poor man's nitric anymore because I have moved on to AP, as many have.
Sodium nitrate.JPG
Dennis
You do not have the required permissions to view the files attached to this post.

jimdoc
Active Member
Posts: 4635
Joined: March 12th, 2007, 10:42 pm
Location: Philadelphia

Re: Processing fingers in poor man's nitric acid

Post by jimdoc » June 16th, 2018, 4:36 pm

This is what I see under last topic with this thread;

Posts
Last post
Re: Processing fingers in poo…

User avatar
FrugalRefiner
Active Member
Posts: 3736
Joined: January 14th, 2012, 5:06 pm
Country of Origin: USA
Location: Ohio, USA

Re: Processing fingers in poor man's nitric acid

Post by FrugalRefiner » June 16th, 2018, 4:41 pm

:lol: Yeah, I see the same thing from the main index page too. :lol:

Dave
Printer friendly copy of C. M. Hoke's Refining Precious Metal Wastes.
Screen readable copy of C. M. Hoke's Refining Precious Metal Wastes.

User avatar
denim
Active Member
Posts: 251
Joined: March 13th, 2012, 10:15 pm
Country of Origin: usa

Re: Processing fingers in poor man's nitric acid

Post by denim » June 16th, 2018, 6:54 pm

Too funny! That did not show up on my phone.

User avatar
Geo
Active Member
Posts: 6423
Joined: March 1st, 2011, 7:56 pm
Country of Origin: U.S.A.
Location: Decatur,Ala.

Re: Processing fingers in poor man's nitric acid

Post by Geo » June 16th, 2018, 8:58 pm

Yea, I saw that too. Totally unintended. :-D Dudadiesel is actually about three miles from my house.
"knowledge is power"
https://www.facebook.com/groups/1778525 ... oup_header
E-WASTE AND PRECIOUS METAL REFINING

User avatar
Geo
Active Member
Posts: 6423
Joined: March 1st, 2011, 7:56 pm
Country of Origin: U.S.A.
Location: Decatur,Ala.

Re: Processing fingers in poor man's nitric acid

Post by Geo » June 16th, 2018, 9:00 pm

Thanks Kurt. I do know about the stump remover but it just didn't cross my mind.
"knowledge is power"
https://www.facebook.com/groups/1778525 ... oup_header