Cyanide found in silver lot shipped to refiner

Post by Jinx86 » August 12th, 2018, 2:34 pm

Recently shipped 3500 ozt of silver to my refiner, the batch tested positive for cyanide. Much of it was already poured into bars for assaying lots prior to purchase. My question is how do I detect cyanide prior to melting or shipping to my refiner. I cannot process the cyanide laiden material in my facility, but would either reject the lot or pass the incurred fees onto the individual sending the material. Also the affected batch would be much smaller and easier to deal with.

User avatar
FrugalRefiner
Active Member
Posts: 3768
Joined: January 14th, 2012, 5:06 pm
Country of Origin: USA
Location: Ohio, USA

Re: Cyanide found in silver lot shipped to refiner

Post by FrugalRefiner » August 12th, 2018, 4:16 pm

I have no personal experience with cyanide, but I can't imagine it would survive melting. Other than the melted and poured bars, what other material did you send?

As far as detecting it, there are a number of commercially available test kits that should do the job. Google something like cyanide test or something along those lines.

Dave
Printer friendly copy of C. M. Hoke's Refining Precious Metal Wastes.
Screen readable copy of C. M. Hoke's Refining Precious Metal Wastes.

jimdoc
Active Member
Posts: 4654
Joined: March 12th, 2007, 10:42 pm
Location: Philadelphia

Re: Cyanide found in silver lot shipped to refiner

Post by jimdoc » August 12th, 2018, 4:28 pm

Was there any cadmium detected?

User avatar
Jinx86
Member
Posts: 5
Joined: November 23rd, 2017, 5:57 pm
Country of Origin: United States
Location: North Dakota

Re: Cyanide found in silver lot shipped to refiner

Post by Jinx86 » August 12th, 2018, 4:34 pm

No cadmium, though I have had issues in the past. This lot would have contained some large batches of jewelry some might have been silver plated or gold plated, also some gold plated franklin mint medals, these are the only items I could image it came from.

Lino1406
Active Member
Posts: 1358
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: Cyanide found in silver lot shipped to refiner

Post by Lino1406 » August 12th, 2018, 11:14 pm

Cyanide test for alkaline solution: 1.Add thiosulphate, this converts cyanide to thiocyanate 2.Add Fe+++ ions, this will give redness by Fe(CNS)3

nickvc
Active Member
Posts: 4228
Joined: September 14th, 2009, 10:53 am
Country of Origin: England
Location: birmingham

Re: Cyanide found in silver lot shipped to refiner

Post by nickvc » August 13th, 2018, 6:52 am

Got to be honest I think your refiner is having a laugh, it sounds to me like your refiner is looking for ways to increase his margins, if the majority was pre melted bars the heat would have destroyed any cyanide and I can’t imagine the coins been a problem as they are struck then plated and rinsed, the plated jewellery would have been rinsed after plating to recover any gold solution.
As an aside I’d keep any gold plated silver aside and melt into individual bar or bars and get them assayed or if you refine use it for inquarting, the gold content should be a nice little bonus which I’m sure your refiner isn’t paying you now.

Lou
Active Member
Posts: 4447
Joined: November 4th, 2007, 5:28 pm
Country of Origin: USA
Location: Rhodia Drive

Re: Cyanide found in silver lot shipped to refiner

Post by Lou » August 13th, 2018, 7:36 am

Ask them to tell you how it tested for cyanide, how much was found and what part of the lot.
Like chemistry? Try http://sciencemadness.org/talk

All that glitters is not gold. Occasionally it's rhodium :)

User avatar
4metals
Active Member
Posts: 4394
Joined: April 5th, 2009, 8:05 pm
Country of Origin: USA
Location: northeast USA

Re: Cyanide found in silver lot shipped to refiner

Post by 4metals » August 13th, 2018, 1:58 pm

Might also be good for our members to know what refiner is telling you this!
Take a trip to our Library, download a copy of Hoke's book for free and learn from previous threads which have been selected and indexed in the library so it is easier to find. Get to the library quickly from; HERE

Lou
Active Member
Posts: 4447
Joined: November 4th, 2007, 5:28 pm
Country of Origin: USA
Location: Rhodia Drive

Re: Cyanide found in silver lot shipped to refiner

Post by Lou » August 13th, 2018, 3:15 pm

Even if it did test, the only thing he did was commit a very big shipping mistake.

Silver cyanide melts to pure silver quite easily with a bit of NO formation (which then becomes NOx, so it does need scrubbed from the flue gas).


Lou
Like chemistry? Try http://sciencemadness.org/talk

All that glitters is not gold. Occasionally it's rhodium :)

nickvc
Active Member
Posts: 4228
Joined: September 14th, 2009, 10:53 am
Country of Origin: England
Location: birmingham

Re: Cyanide found in silver lot shipped to refiner

Post by nickvc » August 13th, 2018, 5:10 pm

4metals wrote:Might also be good for our members to know what refiner is telling you this!
:shock: :D

acpeacemaker
Active Member
Posts: 679
Joined: February 8th, 2011, 6:04 pm
Country of Origin: usa
Location: Colorado

Re: Cyanide found in silver lot shipped to refiner

Post by acpeacemaker » August 13th, 2018, 7:12 pm

Decomposition in the links
HCN
https://www.cdc.gov/niosh/ershdb/emerge ... 50038.html
KCN
https://www.cdc.gov/niosh/ershdb/emerge ... 50037.html
NaCN
https://www.cdc.gov/niosh/ershdb/emerge ... 50036.html
There is spot testing silver cyanide in Feigl, like how Lino explained.
Can also try googling Xray diffraction silver cyanide. These machines are costly.

User avatar
Jinx86
Member
Posts: 5
Joined: November 23rd, 2017, 5:57 pm
Country of Origin: United States
Location: North Dakota

Re: Cyanide found in silver lot shipped to refiner

Post by Jinx86 » August 19th, 2018, 9:56 am

Thanks for all the replies to this so far. I have been in Philadelphia for the ANA show for the last week and will have to give these replies a good read through.