product questions

Formulas
sawmill
Active Member
Posts: 60
Joined: September 19th, 2007, 2:49 am
Location: utah

product questions

Postby sawmill » June 3rd, 2008, 8:41 pm

Hello All
I have a couple questions about some leaching supplies.
Is anyone familiar with a website called Gold mine World?
They have two products that they make some big claims
on for leaching.
One is called Thio-Leach and is a sodium thio sulfate base.
The other is called T6.
Is this just more snake oil,or does it really work?


Lino1406
Active Member
Posts: 1039
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Thiosulphate...

Postby Lino1406 » June 5th, 2008, 12:40 pm

leaches silver from silver chloride (Or
photographic emulsions)

sawmill
Active Member
Posts: 60
Joined: September 19th, 2007, 2:49 am
Location: utah

Postby sawmill » June 6th, 2008, 12:29 am

Lino 1406
Thank you for your reply.
The company that is selling this stuff,claims it
is a good leach,for complex,or gold ore containing
lots of iron,or sulfides.
I just wanted to get some opinions from real refiners,
before getting too excited.

Shaul
Active Member
Posts: 216
Joined: November 29th, 2007, 12:42 am
Country of Origin: USA
Location: Israel

GoldMine World

Postby Shaul » June 6th, 2008, 12:34 am

Sawmill;

Ask Art Corbit about GoldMine World before buying anything from them.

Shaul
You can lead a horse to water but if you can get him to float on his back, then you've really got something.

sawmill
Active Member
Posts: 60
Joined: September 19th, 2007, 2:49 am
Location: utah

Postby sawmill » June 7th, 2008, 3:58 pm

Shaul
Thanks for the reply.
Their advertisement for Thio Leach and T6
sounded reasonable. But after reading their
stuff about getting 8 ounces of gold from a
ton of alfalfa,mining water wells,and refining
table salt,the bells went off. :shock:
Since my pointy hat and cape is at the cleaners,
and I lost my wand,maybe I can't use that stuff. :lol:


User avatar
Irons
Active Member
Posts: 1670
Joined: September 8th, 2007, 2:59 pm
Location: Dark side of the Moon

Postby Irons » June 7th, 2008, 4:09 pm

sawmill wrote:Shaul
Thanks for the reply.
Their advertisement for Thio Leach and T6
sounded reasonable. But after reading their
stuff about getting 8 ounces of gold from a
ton of alfalfa,mining water wells,and refining
table salt,the bells went off. :shock:
Since my pointy hat and cape is at the cleaners,
and I lost my wand,maybe I can't use that stuff. :lol:


But then, the Alfalfa had to be growing on soil that was 75% Gold by weight. :P
The stingy man pays the most.

I cut it 3 times and it's still too short.

sawmill
Active Member
Posts: 60
Joined: September 19th, 2007, 2:49 am
Location: utah

Postby sawmill » June 7th, 2008, 4:35 pm

Irons
That is a good idea. I will just plant my
claims in alfalfa. Throw all that mining
stuff away and get a hay baler. Sure
would save on lots of digging in the hot
sun and rattlesnakes. :shock: :D :D :D :D

watlarry
Member
Posts: 25
Joined: February 17th, 2008, 4:14 pm
Location: usa

Re: product questions

Postby watlarry » June 7th, 2008, 6:58 pm

sawmill wrote:Hello All
I have a couple questions about some leaching supplies.
Is anyone familiar with a website called Gold mine World?
They have two products that they make some big claims
on for leaching.
One is called Thio-Leach and is a sodium thio sulfate base.
The other is called T6.
Is this just more snake oil,or does it really work?


I used Thio-Leach on a batch of pins. Sat in a bucket with an air bubbler
for weeks .......no results.
That was before I found this site. drained them rinsed them a put them
in a batch of AP. Thats how you get stuff done.

Thank you,
Steve and everyone responsible for site.
larry

Shecker
Active Member
Posts: 241
Joined: April 1st, 2008, 10:34 am
Location: Gunnison, Colorado
Contact:

T-6

Postby Shecker » June 29th, 2008, 1:45 pm

I once went to Mike's lab and was not impressed. He poured some of his T-6 into a solution, made a green precipitate, and declared it to be rhodium. I said that it didn't look like rhodium to me. He swore it was rhodium but offered no means of checking that out. Frankly T-6 does not impress me and it smells bad. There are other thingsd I would rather use.

Randy in Gunnison
Gold and Silver are the basis of a sound economy.
Economic strength comes from fair weights and measures.

Lino1406
Active Member
Posts: 1039
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Green rhodium

Postby Lino1406 » June 29th, 2008, 2:15 pm

There are numerous agents which
precipitate rhodium as a complex.
So you can't rule that out.

Lino1406
Active Member
Posts: 1039
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

That includes..

Postby Lino1406 » June 29th, 2008, 2:39 pm

Also some other PM's, since maybe
the man could have referred to Palladium, Iridium
(called by some E-rhodium) etc.

Shecker
Active Member
Posts: 241
Joined: April 1st, 2008, 10:34 am
Location: Gunnison, Colorado
Contact:

T-6

Postby Shecker » June 29th, 2008, 4:04 pm

My understanding of T-6 is that precipitates everything as a green complex.
Even the gold comes out green. With his older Big Red product the pgm's dropped black and gold yellow. At least that gave you idea of which way was up. But everything green -- looks like I did the last time I had a stomach virus.

Randy in Gunnison
Gold and Silver are the basis of a sound economy.

Economic strength comes from fair weights and measures.

Lino1406
Active Member
Posts: 1039
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Rhodium (and others') precipitants

Postby Lino1406 » June 29th, 2008, 11:06 pm

A partial list:
Thioacetamide
Hydroxylamine
TiCl3