This category is for Precious Metals related Refiners, Scrap Buyers, Scrap Processors, Assayers, etc. It is the only place on the forum where these companies or individuals can pitch their commercial services. Warning: If this is done in any other forum category, it will be considered spam and will be deleted.
Post Reply
Lino1406
Active Member
Posts: 1586
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

30 and more recovery procedures - New edition

Post by Lino1406 » December 14th, 2013, 10:55 am

List of contents: page
1. The fixer from photography, silver bearing solution 2
2. The silver cyanide solution 3
2a. The 'out taker' powder for precipitating from cyanide solution 3
3. The wet silver chloride scrap 3
4. Dry silver chloride/bromide/iodide 4
5. Silver nitrate, dry or in solution 4
6. Silver plating 4
7. Silver from the silver chloride -mercury chloride mixture 5
8. Silver from the silver chloride -mercury chloride mixture containing
organic matter 5
9. Silver from the silver-zinc battery 5
gold recycling: forward 6
10. Gold cyanide solution 6
10a. The 'out taker' powder 7
11. Acidic gold (either gold ammonium sulphite or gold chloride) 7
12. Acidic gold (aqua regia solution where other metals are present) 7
13. Gold from the iodine/iodide solution, mercury amalgam 8
14. Gold from the electronic scrap 8
15. Palladium from the cyanide solution 9
15a. The 'out taker' powder 9
16. Palladium from the acidic solution 9
17. Palladium from the palladium on charcoal catalyst 10
18. Palladium from the Mercury-Copper-palladium amalgam. 11
19. Platinum from the acidic solution 11
20. Platinum from the Pt on charcoal catalyst 12
21. Rhodium from the acidic Rh solution 12
22. Rhodium from the Rh over charcoal catalyst 12
23. Platinum, palladium and rhodium from the cat honeycomb converter 12
24. Osmium dioxide and osmium from the osmium tetroxide scrap 13
25. Non selective extraction of acidic solution containing precious metals 13
26. Rhenium from potassium perrhenate 14
27. Ruthenium from the Ru plating solution 15
28. The nano-gold, nano-silver, nano- palladium dispersion 15
29. Recovery from organo metal complexes 16
30. Short cut. Platinum, palladium and other PM's from their oxides 16
obtain through Paypal - $8.50 (give e-mail address)
Last edited by Lino1406 on June 16th, 2014, 11:55 am, edited 2 times in total.

galenrog
Active Member
Posts: 417
Joined: January 16th, 2010, 4:54 pm
Country of Origin: USA
Location: Oregon

Re: 30 and more recovery procedures - New edition

Post by galenrog » December 14th, 2013, 5:03 pm

Should this be on the sale page rather than the refining page?
Mine gold. Buy silver. Fills the safe faster.

User avatar
goldsilverpro
Active Member
Posts: 7962
Joined: March 30th, 2007, 4:45 pm
Country of Origin: USA
Location: Benton, Arkansas

Re: 30 and more recovery procedures - New edition

Post by goldsilverpro » December 14th, 2013, 5:11 pm

Should this be on the sale page rather than the refining page?
It's in the right place. Among other things, the refiner's category has been sort of a catch-all for people selling refining books. For example, it's where I put the ad for my book. Let the moderators deal with this sort of thing.
"Everything should be as simple as possible, but not simpler" - Albert Einstein
"It is better to hear the rebuke of the wise, than for a man to hear the song of fools" Ecc 7:5, 1611 AV
"The refiner is always the last liar." Louis Labash, 1979

GoldSilverPro's eBook For Sale. http://goldrefiningforum.com/phpBB3/vie ... 17#p233617
GSP Consulting http://goldrefiningforum.com/phpBB3/vie ... 84&t=26425

galenrog
Active Member
Posts: 417
Joined: January 16th, 2010, 4:54 pm
Country of Origin: USA
Location: Oregon

Re: 30 and more recovery procedures - New edition

Post by galenrog » December 15th, 2013, 11:08 am

Thank you, GSP, for reminding me. My apologies to the OP.
Mine gold. Buy silver. Fills the safe faster.

Lino1406
Active Member
Posts: 1586
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: 30 and more recovery procedures - New edition

Post by Lino1406 » October 24th, 2014, 7:35 am

What do the drifting prices foresee?
Hopefully the world does not proceed into a slowdown where
all assets are down and let the recovery procedures remain relevant
Last edited by Lino1406 on November 2nd, 2014, 10:22 pm, edited 1 time in total.

User avatar
4metals
Active Member
Posts: 4423
Joined: April 5th, 2009, 8:05 pm
Country of Origin: USA
Location: northeast USA

Re: 30 and more recovery procedures - New edition

Post by 4metals » October 24th, 2014, 12:04 pm

Lino,

I have developed respect for your knowledge from reading your posts on the forum, thank you for that.

Can you post some details as to how members can obtain this document from you?
Take a trip to our Library, download a copy of Hoke's book for free and learn from previous threads which have been selected and indexed in the library so it is easier to find. Get to the library quickly from; HERE

Lino1406
Active Member
Posts: 1586
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: 30 and more recovery procedures - New edition

Post by Lino1406 » October 25th, 2014, 12:58 pm

Thanks 4metals. The e-booklet is sent by e-mail (word format).
It contains some information not included in other sources.
An e-mail address is needed for charging through PP.
Price remains unchanged.

antikmes
Member
Posts: 1
Joined: January 3rd, 2017, 10:57 am
Country of Origin: azerbijan

Re: 30 and more recovery procedures - New edition

Post by antikmes » November 24th, 2017, 11:05 am

I read this booklet and it is well organized, inclusive despite its seemingly shortness. May be worth its price many times for every PM’s reclaimer, as well as saving much money for one who is not sure enough if to enter this field at all.

Lino1406
Active Member
Posts: 1586
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: 30 and more recovery procedures - New edition

Post by Lino1406 » December 5th, 2017, 10:30 pm

Antikmes wrote:
I read this booklet and it is well organized, inclusive despite its seemingly shortness. May be worth its price many times for every PM’s reclaimer, as well as saving much money for one who is not sure enough if to enter this field at all.

That's certainly a good point.
Thank you