This category is for Precious Metals related Refiners, Scrap Buyers, Scrap Processors, Assayers, etc. It is the only place on the forum where these companies or individuals can pitch their commercial services. Warning: If this is done in any other forum category, it will be considered spam and will be deleted.
Post Reply
User avatar
Nuwaysolutions
Member
Posts: 32
Joined: November 1st, 2016, 12:52 pm
Country of Origin: usa

Smopex for sale on EBay?

Post by Nuwaysolutions » November 29th, 2017, 2:58 pm

Does anyone know much about smopex? It’s supposed to pick up gold and platinum group metals. I looked online and it seems to be pretty expensive stuff like $15-$20 a gram. It’s $5 on eBay which seems reasonable if it works. If anyone has any info or experience with it please share. Thanks for any help.


Sent from my iPhone using Tapatalk

jimdoc
Active Member
Posts: 4769
Joined: March 12th, 2007, 10:42 pm
Location: Philadelphia

Re: Smopex for sale on EBay?

Post by jimdoc » November 29th, 2017, 3:04 pm


User avatar
Palladium
Active Member
Posts: 5349
Joined: January 17th, 2008, 1:54 am
Location: USA

Re: Smopex for sale on EBay?

Post by Palladium » November 29th, 2017, 3:09 pm

Wow! This made my head hurt!

https://www.google.com/patents/US7687663
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C.M. Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/y9w5y73
4. Silver cell setup video here (FREE) >> https://tinyurl.com/jhzadse
ALL FREE-----ALL THE TIME

User avatar
Palladium
Active Member
Posts: 5349
Joined: January 17th, 2008, 1:54 am
Location: USA

Re: Smopex for sale on EBay?

Post by Palladium » November 29th, 2017, 3:20 pm

An interesting read. :arrow:
You do not have the required permissions to view the files attached to this post.
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C.M. Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/y9w5y73
4. Silver cell setup video here (FREE) >> https://tinyurl.com/jhzadse
ALL FREE-----ALL THE TIME

snoman701
Active Member
Posts: 1608
Joined: October 8th, 2016, 10:24 pm
Country of Origin: USA
Location: SE MI

Re: Smopex for sale on EBay?

Post by snoman701 » November 29th, 2017, 3:29 pm

Smopex has been discussed on the board before, so there's a reasonable amount of information here as well.

The price as advertised on the board previously was 60-200 USD / kg, so obviously that's changed a bit.

User avatar
Nuwaysolutions
Member
Posts: 32
Joined: November 1st, 2016, 12:52 pm
Country of Origin: usa

Re: Smopex for sale on EBay?

Post by Nuwaysolutions » November 29th, 2017, 3:33 pm

Thanks for the info. May try a sample.


Sent from my iPhone using Tapatalk

User avatar
Palladium
Active Member
Posts: 5349
Joined: January 17th, 2008, 1:54 am
Location: USA

Re: Smopex for sale on EBay?

Post by Palladium » December 2nd, 2017, 12:13 am

He's dropped the price in half! It's $2.50 a gram now.
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C.M. Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/y9w5y73
4. Silver cell setup video here (FREE) >> https://tinyurl.com/jhzadse
ALL FREE-----ALL THE TIME

User avatar
Palladium
Active Member
Posts: 5349
Joined: January 17th, 2008, 1:54 am
Location: USA

Re: Smopex for sale on EBay?

Post by Palladium » December 2nd, 2017, 12:14 am

The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C.M. Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/y9w5y73
4. Silver cell setup video here (FREE) >> https://tinyurl.com/jhzadse
ALL FREE-----ALL THE TIME

User avatar
Nuwaysolutions
Member
Posts: 32
Joined: November 1st, 2016, 12:52 pm
Country of Origin: usa

Re: Smopex for sale on EBay?

Post by Nuwaysolutions » December 2nd, 2017, 12:18 am

I asked for a sample and he’s sending me 5 grams for $5 shipping. I’ll post in about 2 weeks on if it works.


Sent from my iPhone using Tapatalk

User avatar
g_axelsson
Active Member
Posts: 5086
Joined: November 17th, 2007, 8:46 pm
Location: Sweden

Re: Smopex for sale on EBay?

Post by g_axelsson » December 2nd, 2017, 6:42 am

Smopex 105...
Recovery of negatively charged precious metals complexes used in complex reactions (Suzuki, Heck, Sonagashira). Recovery of precious metals from catalyst process streams, especially Pd, Rh, Ru, Pt, Ir, and Os. Also, heavy metals removed: Re, Au, Ag, Fe, Co, Cu, Sn, Cd, Ni, Pb, Cr, Zn, V, and Hg. Removal of alkyl and benzyl metal halides.
Sounds pretty useless to refining to me, just crash every metal out as a hydroxide if that is what you want. Even cementing on iron would produce a more pure product without the hassle of incinerating the polymers afterwards.
Smopex 105 has it's use in organic chemistry where you want to remove a metal catalyst from your finished product.

Using Smopex 105 for refining seems to be like using a wrench to hammer down a screw into a wooden board. You can do it but the result would be better if you used cheaper tools in a proper way.