This category is for Precious Metals related Refiners, Scrap Buyers, Scrap Processors, Assayers, etc. It is the only place on the forum where these companies or individuals can pitch their commercial services. Warning: If this is done in any other forum category, it will be considered spam and will be deleted.
Post Reply
Lino1406
Active Member
Posts: 1717
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

37 recovery procedures - E-booklet. $8.50

Post by Lino1406 » May 31st, 2018, 11:08 pm

Reclaiming PM's safely and ecologically
in the scrapyard

37 cases of precious metals reclamation


by: Arik Lin, Ph.D.
You do not have the required permissions to view the files attached to this post.

Lino1406
Active Member
Posts: 1717
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: 37 recovery procedures - E-booklet. $8.50

Post by Lino1406 » January 26th, 2019, 2:20 pm

Not sleeping while standing up...never stop updating.
Here are some of the recent updates:
How tin dioxide is dissolved?
Under which conditions A/P dissolves gold?
Recover gold from GaAs mos-fets
All recovery answers under one roof (point questions are answered on the forum)