Post by cleanbucket1 » January 14th, 2012, 5:50 pm

Hello. Always looking for new things to discover gold in and maybe some of you that have been doing this for a while can help.
Obviously you wouldnt want to collect these from anyone you do not know for the fear of self contamination of diseases, BUT, if anyone has them, the plastic pieces you have to replace every so often have 2- 4 gold fingers on them depending on the tester. HEY, GOLD IS GOLD RITE....
Also, the strips themselves seem to have gold routes such as a computer board does with copper. Not all types but the ones my Gramms uses does. These have a thin clear layer of plastic over them that has to come off ( I soak them in soap and hot water. Not sure if that on the strips is recoverable gold, but when I find out ill let you know, Or if anyone else has an explanation, PLEASE, im all ears. I have not yet tried to process.

User avatar
samuel-a
Active Member
Posts: 2147
Joined: October 7th, 2009, 1:26 am
Country of Origin: Il
Contact:

Re: Diabetes strips (gold )

Post by samuel-a » January 14th, 2012, 7:19 pm

Yes, the strips have plated gold on traces of some conductive mylar as well as contact points.
easly recognizable.

The silvery looking one are Pd.
Regards, Sam

http://www.goldnscrap.com | I'm on Google+ and Twitter too....

GNS - e-scrap yield list v1.0 (link fixed)

User avatar
cleanbucket1
Member
Posts: 41
Joined: January 14th, 2012, 2:45 pm
Country of Origin: usa

Re: Diabetes strips (gold )

Post by cleanbucket1 » January 15th, 2012, 12:59 am

Very nice. Thank you samuel. You wouldnt happen to know any kind of yield by weight ratio on this material would you? On the gold that is..

User avatar
samuel-a
Active Member
Posts: 2147
Joined: October 7th, 2009, 1:26 am
Country of Origin: Il
Contact:

Re: Diabetes strips (gold )

Post by samuel-a » January 15th, 2012, 2:03 am

Never had enough of it to come up with a number...

Also, there are so many manufacturers... even if i had the numbers, they would have been worthless.
Regards, Sam

http://www.goldnscrap.com | I'm on Google+ and Twitter too....

GNS - e-scrap yield list v1.0 (link fixed)

User avatar
cleanbucket1
Member
Posts: 41
Joined: January 14th, 2012, 2:45 pm
Country of Origin: usa

Re: Diabetes strips (gold )

Post by cleanbucket1 » January 16th, 2012, 10:56 am

LOL. Thats so very true. My grams saves hers for me, so I get the same ones each time. In the future when I get them all together and run a batch ill share the info. Probably wait til I get atleast 1 pound.
Thanks for your time.

User avatar
gold4mike
Active Member
Posts: 678
Joined: February 9th, 2009, 2:19 pm
Country of Origin: USA
Location: Ohio

Re: Diabetes strips (gold )

Post by gold4mike » January 16th, 2012, 11:08 am

I'm glad I bumped into this thread. I recently bought about 50 Blood Glucose test units at an auction that include a base unit, a hand held smaller unit and many bottles of the unused test strips. There's no visible gold on the test strips but the units each contain 4 circuit boards and the connectors are fully plated.

I'll try to separate the layers on the test strips and see what I can find.

Thanks!
The problems we face today exist because the people who work for a living are outnumbered by those who vote for a living.

User avatar
etack
Active Member
Posts: 1312
Joined: November 8th, 2008, 11:41 pm
Country of Origin: usa
Location: Dayton, Ohio
Contact:

Re: Diabetes strips (gold )

Post by etack » January 16th, 2012, 11:48 pm

hey Mike in Dayton on craigslist a person will buy them from you.

http://dayton.craigslist.org/hab/2780336240.html


Eric
As Harold says "Read Hoke be enlightened"

Will buy your tantalum capacitors send a PM for price buy the pound.

http://goldrefiningforum.com/phpBB3/vie ... 59&t=15909

A simple search of the forum would have given you the answers without posting.

User avatar
Jason1
Member
Posts: 43
Joined: December 10th, 2011, 8:09 pm
Country of Origin: US
Location: Upstate SC
Contact:

Re: Diabetes strips (gold )

Post by Jason1 » January 17th, 2012, 12:31 am

cleanbucket1 wrote: Also, the strips themselves seem to have gold routes...Not all types but the ones my Gramms uses does
Right, from what I gather, not all of them use Gold.My dad was using OneTouch Ultra which doesn't "appear" to have any sort of Gold plating on the strips (but may have some other sort of metal worth saving, I don't know). Now, he uses Accu-Chek strips, which clearly have Gold/Gold plated contacts. Just one more reason to stay after him about his blood sugar lol.




cleanbucket1 wrote: ...Not sure if that on the strips is recoverable gold...
I processed some of the latter strips along with some other gold plated items so I couldn't say whether they're "recoverable," but I do know the gold comes off in AP. Being so thin, they have a nasty habit of getting stuck together as well.

User avatar
samuel-a
Active Member
Posts: 2147
Joined: October 7th, 2009, 1:26 am
Country of Origin: Il
Contact:

Re: Diabetes strips (gold )

Post by samuel-a » January 17th, 2012, 12:46 am

Jason1 wrote:Being so thin, they have a nasty habit of getting stuck together as well.
I totally forgot about it.
A 30 minutes soak in plain hot water will relive it from all of the gooey paste. The water will turn yellow IIRC.
Then, direct AR/HCl+Cl.
Regards, Sam

http://www.goldnscrap.com | I'm on Google+ and Twitter too....

GNS - e-scrap yield list v1.0 (link fixed)

User avatar
Jason1
Member
Posts: 43
Joined: December 10th, 2011, 8:09 pm
Country of Origin: US
Location: Upstate SC
Contact:

Re: Diabetes strips (gold )

Post by Jason1 » January 17th, 2012, 1:17 am

samuel-a wrote: I totally forgot about it.
A 30 minutes soak in plain hot water will relive it from all of the gooey paste.
I will remember to do that in the future. Thanks
samuel-a wrote: The water will turn yellow IIRC.

What's IIRC? (I'm new to this)

samuel-a wrote:
Then, direct AR/HCl+Cl.
AR, Is that right? or did you mean AP? (Again, I'm a newbie, so sorry about all the questions)

Jason

User avatar
Geo
Active Member
Posts: 6527
Joined: March 1st, 2011, 7:56 pm
Country of Origin: U.S.A.
Location: Decatur,Ala.

Re: Diabetes strips (gold )

Post by Geo » January 17th, 2012, 1:35 am

AR = Aqua Regia

AP = acid(hcl) + peroxide(will not dissolve gold unless excess amounts of peroxide is used and then only small amounts will dissolve).

hcl/cl = hcl acid (muriatic acid) + chlorine (household bleach,sodium hypochlorite)

if you are familiar with aqua regia then use that, if you are familiar with hcl/cl then this will work equally as well. if you don't know one or the other of these two processes then you should study the reactions and practice using them as both are very good tools to have your inventory.

oh yea,IIRC is an abbreviation for "if i remember correctly" which is not to be confused with texting lingo.
"knowledge is power"
https://www.facebook.com/groups/1778525 ... oup_header
E-WASTE AND PRECIOUS METAL REFINING

User avatar
Jason1
Member
Posts: 43
Joined: December 10th, 2011, 8:09 pm
Country of Origin: US
Location: Upstate SC
Contact:

Re: Diabetes strips (gold )

Post by Jason1 » January 17th, 2012, 1:52 am

Oh, ok. He was saying AR or HCl+Cl. I got it. Thanks

jack_burton
Active Member
Posts: 205
Joined: December 18th, 2011, 1:40 am
Country of Origin: United States
Location: Pennsylvania, USA

Re: Diabetes strips (gold )

Post by jack_burton » January 17th, 2012, 7:43 am

Well as a side note, it would explain why they are so expensive... I'm a type II diabetic- my strips are around $100 a month, depending how often I check. Guess I'll start a new stockpile to get my money back! :shock:
____________________________________________
JB

____________________________________________

User avatar
jimmydolittle
Active Member
Posts: 157
Joined: September 15th, 2011, 6:55 pm
Country of Origin: USA
Location: Southern Indiana

Re: Diabetes strips (gold )

Post by jimmydolittle » January 17th, 2012, 8:09 am

My wife at one time had a meter that had the gold fingered test strips, I can't remember what it was called. As I recall, the strips had an indent where the finger was placed to take the sample. She has had several over the years.
If it’s difficult, we do it immediately, if it’s impossible, then it just takes a little longer.

bigredlee
Member
Posts: 7
Joined: January 15th, 2014, 3:59 pm
Country of Origin: USA
Location: Rochester, NY

Re: Diabetes strips (gold )

Post by bigredlee » January 22nd, 2014, 1:50 pm

I am reading through this and anything that comes in contact with blood is a real safety concern. I work in the sterilization industry and I would never touch these with my bare hands pre-sanitization. The industry standard is 180F for 180s minimum in a wet environment(boil them for five minutes for good measure.) This will kill any living pathogen, although it will not denature the proteins in the spores, so it will never be sterile in boiling water. The A/P should do the trick to chemically sterilize though, wear your latex gloves!!

User avatar
solar_plasma
Active Member
Posts: 2693
Joined: February 27th, 2013, 12:37 pm
Country of Origin: germany
Location: Germany

Re: Diabetes strips (gold )

Post by solar_plasma » November 11th, 2014, 11:25 pm

bigredlee wrote:I am reading through this and anything that comes in contact with blood is a real safety concern. I work in the sterilization industry and I would never touch these with my bare hands pre-sanitization. The industry standard is 180F for 180s minimum in a wet environment(boil them for five minutes for good measure.) This will kill any living pathogen, although it will not denature the proteins in the spores, so it will never be sterile in boiling water. The A/P should do the trick to chemically sterilize though, wear your latex gloves!!
If you get those from unknown sources/people, incineration would be the most safe and clean pretreatment. Since I get my material only from family members, I am fine with standard lab hygiene and straight AR.
Best regards
Björn
Disclaimer
Everything I write on the forum regardless the wording may contain false or incomplete statements and is a matter of theoretical exchange of insights and assumptions for an educational purpose. I do not advise to use anything of it in practice, and if you use it anyway, you do it on your own risk and responsibility provided that you have the professional knowledge to do it safely and only if permitted to you by the respective laws of your country.

alexsalter3d
Member
Posts: 10
Joined: January 26th, 2015, 3:51 pm
Country of Origin: United Kingdom

Re: Diabetes strips (gold )

Post by alexsalter3d » January 26th, 2015, 4:08 pm

AHAHAHAHa -i'm type 1. Looks like i've just found a use for the like, 9 Testes I do a day then, lmao

User avatar
solar_plasma
Active Member
Posts: 2693
Joined: February 27th, 2013, 12:37 pm
Country of Origin: germany
Location: Germany

Re: Diabetes strips (gold )

Post by solar_plasma » January 26th, 2015, 5:37 pm

There is another thread about this you should read. The incredible yield two members posted in the beginning has never been confirmed though. I think they have not been active for a long time anymore. Expect about 1g from about 2400 pieces, if they are golden.

http://goldrefiningforum.com/~goldrefi/ ... 60&t=16336
Best regards
Björn
Disclaimer
Everything I write on the forum regardless the wording may contain false or incomplete statements and is a matter of theoretical exchange of insights and assumptions for an educational purpose. I do not advise to use anything of it in practice, and if you use it anyway, you do it on your own risk and responsibility provided that you have the professional knowledge to do it safely and only if permitted to you by the respective laws of your country.

Shaul
Active Member
Posts: 218
Joined: November 29th, 2007, 12:42 am
Country of Origin: USA
Location: Israel

Re: Diabetes strips (gold )

Post by Shaul » February 14th, 2015, 5:56 pm

The Accu Chek test strips (the ones with two silver-colored metallic strips) contain Palladium.

Shaul
You can lead a horse to water but if you can get him to float on his back, then you've really got something.

User avatar
jeneje
Active Member
Posts: 1176
Joined: January 23rd, 2011, 1:51 pm
Country of Origin: USA
Location: Knoxville Tennessee
Contact:

Re: Diabetes strips (gold )

Post by jeneje » February 14th, 2015, 6:34 pm

Here is a great source for Accu Chek Test Strips-Fire Assay Data.
http://refinementofpreciousmetals.com/v ... =140&t=901
Ken
Never jump in blind, it's leads to stupidity!
My mind works like lightning - One brilliant flash and it's GONE!!
The difference between Stupidity and Wisdom - Wisdom lets' Stupidity go first!


http://www.refinementofpreciousmetals.com

artart47
Active Member
Posts: 547
Joined: February 9th, 2010, 4:01 am
Country of Origin: usa
Location: North Cape, wi

Re: Diabetes strips (gold )

Post by artart47 » February 14th, 2015, 6:50 pm

Hi friends!
I have a number of people saving them for me and while working on the old nursing home my friend bought in Peshtigo, wisconsin I discovered "the dirty room" It is filled with huge cardboard boxes containing containers of bio waste. Seringes and more test strips than racine has "obama phones"
I'll be bringing it back with me along with any medical devices that they're not going to use. These strips are about a quarter inch x about an inch and a quarter. Is that the size of them. I've seen pics on the posts but with nothing to reference the size. Always thought they were really big.
Been reading a lot about them and plan to see what comes from them.

artart47

User avatar
FrugalRefiner
Active Member
Posts: 4353
Joined: January 14th, 2012, 5:06 pm
Country of Origin: USA
Location: Ohio, USA

Re: Diabetes strips (gold )

Post by FrugalRefiner » February 14th, 2015, 7:33 pm

Art, please be very careful with that stuff. You'll potentially be exposed to every nasty disease that's come through that facility.

Dave
Printer friendly copy of C. M. Hoke's Refining Precious Metal Wastes.
Screen readable copy of C. M. Hoke's Refining Precious Metal Wastes.

User avatar
solar_plasma
Active Member
Posts: 2693
Joined: February 27th, 2013, 12:37 pm
Country of Origin: germany
Location: Germany

Re: Diabetes strips (gold )

Post by solar_plasma » February 15th, 2015, 12:35 am

Remember, there is only gold on those you can see gold traces and it takes 2400 pieces for one gramm gold. If they aren't collected by kind in safe boxes and if they are just mixed with and thrown to the other waste, - let it be. It is not worth the risk.
Best regards
Björn
Disclaimer
Everything I write on the forum regardless the wording may contain false or incomplete statements and is a matter of theoretical exchange of insights and assumptions for an educational purpose. I do not advise to use anything of it in practice, and if you use it anyway, you do it on your own risk and responsibility provided that you have the professional knowledge to do it safely and only if permitted to you by the respective laws of your country.

artart47
Active Member
Posts: 547
Joined: February 9th, 2010, 4:01 am
Country of Origin: usa
Location: North Cape, wi

Re: Diabetes strips (gold )

Post by artart47 » February 15th, 2015, 9:14 am

Hi!
Thanks for the warnings! I'll be very careful! My idea is to take each container and immerse them in a steel drum with a wood fire under it and bring it to an extended boil. Before attempting to screen out the test strips. Or just incinerate the contents of each container as I remove it from the boxes. any suggestions are welcome.
Thanks again. artart47

Barren Realms 007
Active Member
Posts: 4598
Joined: April 2nd, 2009, 3:46 pm
Country of Origin: US
Location: Arkansas
Contact:

Re: Diabetes strips (gold )

Post by Barren Realms 007 » February 15th, 2015, 1:07 pm

artart47 wrote:Hi!
Thanks for the warnings! I'll be very careful! My idea is to take each container and immerse them in a steel drum with a wood fire under it and bring it to an extended boil. Before attempting to screen out the test strips. Or just incinerate the contents of each container as I remove it from the boxes. any suggestions are welcome.
Thanks again. artart47
Incineration is your only safe option, even then I feel you might be in some danger of contamination of what you breath. I know you are really wanting to tackle this project but I feel strongly it is one you should walk away from.
Give a man a fish and you feed him for a day, teach a man to fish and you feed him for life.
You have to crawl before you can walk.
Patience is a virtue.
A man has got to know his limitations.

Chance favors the prepared

Post Reply