home made cupels

qst42know
Active Member
Posts: 2963
Joined: July 16th, 2008, 12:31 am
Country of Origin: USA
Location: Toledo, Ohio, USA

Post by qst42know » October 17th, 2008, 6:14 pm

Mortar mix already has sand in it. You must find plain Portland cement. It will be marked as such. It is the binder in concrete and mortar mix. I bought an 80# bag several years ago at Home Depot for about $6. I am still working from that bag. Controlling the moisture to make these is vital to prevent splitting.
I have also used straight Vigoro brand bone meal from the garden center. These work in smaller sizes just pressed with no additives and then roasted to ash to drive off the fats present. These will smell bad a lot like burning hair. Roasting after pressing reveals the ones that will split in use. They soak lead like nobodies business but are limited to about 1"diameter or less. Larger sizes will need a binder of some sort.

bmgold
Active Member
Posts: 183
Joined: September 28th, 2008, 10:46 am
Location: Pennsylvania

Post by bmgold » October 18th, 2008, 9:53 am

Yes, you are right about the sand. I got the mortar mix for free since the bag was ripped and spilled. That would explain the glassy look when I tried cupelling a small test.

I got some store bought (action mining) cupels and tried one out with the torch. One problem I am having is silver. I want the nice gold color in my tiny beads but after trying a larger sample I think I have silver since there was a considerable amount of "sprouting" on my last attempt. Either my lead I used was contaminated with silver or my melting cup (made from cement a year or so ago) is contaminating my tests with silver from previous tests (likely).

I did try the straight bone MEAL and it did work but smelled bad and again a tiny silver colored bead. I have no nitric acid and won't pay the hazardous shipping fee to get some so I have no way that I know of to part the beads. They are mostly almost microscopic except for the last one. I've been saving all my tiny cupels to someday recover the precious metals and hopefully even the lead. I've tested the lead oxide layer in some with a reducing flame and can get the lead to reform into metal form again. I don't want to just throw them away since they contain some gold/silver/etc. and I figure the lead oxide is probably more dangerous than the lead metal. No since contaminating the Earth any more than I have to. The lead does form some really pretty colors on the sides of the cupels. I can see why it was/is used in paints.

Thanks for the great forum full of great knowledge and great people. Keep it up everyone.

qst42know
Active Member
Posts: 2963
Joined: July 16th, 2008, 12:31 am
Country of Origin: USA
Location: Toledo, Ohio, USA

Post by qst42know » October 18th, 2008, 1:47 pm

The text I have on the subject is: "A Manual Of Fire Assaying by Charles Herman Fulton". This was a college text from Penn State back in 1911. The older texts have much more info on making your own stuff, from furnace construction for several types of fuel, to making cupels, and formulating your own fluxes. The commercial made cupels are likely more reliable for accurate scientific assaying, but for experimenting with the process home made will work fine. This book is well worth looking for. You may be able to find it at your local library.

butcher
Active Member
Posts: 9071
Joined: January 6th, 2008, 2:09 pm
Country of Origin: USA
Location: Pacific NW

Post by butcher » October 19th, 2008, 8:59 am

bmgold read this forum for ways to make your nitric for parting,

jimdoc
Active Member
Posts: 4769
Joined: March 12th, 2007, 10:42 pm
Location: Philadelphia

A Manual Of Fire Assaying

Post by jimdoc » October 19th, 2008, 3:52 pm

Here is a link to that book;

http://www.archive.org/details/manualof ... 00fultiala

There are also alot of the older books on the site.

Jim

bmgold
Active Member
Posts: 183
Joined: September 28th, 2008, 10:46 am
Location: Pennsylvania

Post by bmgold » October 19th, 2008, 4:20 pm

Thanks for the link to the book and the link to e-bay nitric acid. The nitric was expensive but the shipping was WAY less than other places I checked. Probably won't be buying any but it's nice to know it is there. As for the book, I have it downloading now. This forum is full of great people!!!

Back to the homemade cupels and my silver problem: I still think I have silver but not as much as I thought. My lead "sprouted" as it cooled down when I moved the torch away before the process was done. I thought only pure silver would do this but I seem to be wrong (Admitting it is the first step to a solution) My real problem is I'm just working with too small amounts of precious metals. With a magnifying glass and good light I can find TINY beads in the cupels, both the homemade and the store bought ones so I just have to back up and start over. The process does work and it don't make gold where there is none. I'm probably the only one on the forum that tried to get to the end product too quick.

Thanks again everyone for making this kind of information available for little more than the cost of time to read and study.

User avatar
viacin
Active Member
Posts: 344
Joined: September 30th, 2008, 6:25 pm
Location: Alabama, USA

Post by viacin » October 19th, 2008, 4:52 pm

bmgold wrote: link to e-bay nitric acid.
:?: Where is said link? I would like to see this. I've searched a few times but found nothing.
Of all the contrivances for cheating the laboring classes of mankind, none has been more effective than that which deludes them with paper money. - Daniel Webster

qst42know
Active Member
Posts: 2963
Joined: July 16th, 2008, 12:31 am
Country of Origin: USA
Location: Toledo, Ohio, USA

Post by qst42know » October 19th, 2008, 5:40 pm

If your flux is balanced and your assay is going correctly your PM will be quite pure, nearly round and sitting just barely touching the cupel, it will be attached but not strongly. Almost like a bb in a teacup. If your bead of metal is flat and firmly bonded to the cupel it is a sign that you havent removed all the base metals.

bmgold
Active Member
Posts: 183
Joined: September 28th, 2008, 10:46 am
Location: Pennsylvania

Post by bmgold » October 19th, 2008, 7:09 pm

I guess I should have ordered it when I saw it (E-bay nitric) I can't find it again either and I don't even see the message I got the item number from.

Maybe I made it up or maybe I've been breathing too many lead fumes :?

It was from a company that also sold biodiesel making supplies. Maybe if somebody really posted then deleted the message they can jump back in with more info. I think the listing was ended but there was other auctions or buy it now sales (I thought)

qst42know
Active Member
Posts: 2963
Joined: July 16th, 2008, 12:31 am
Country of Origin: USA
Location: Toledo, Ohio, USA

Post by qst42know » October 19th, 2008, 7:29 pm

I looked at the nitric acid auctions when the subject first came up. Now they don't even show on the completed side (and it has not been that long ago) which tells me the auctions were scrubbed by eBay perhaps by governmental request.

Shades of big brother.

Without a buisness that requires it, You'll have to make what you need. Till they put a stop to that as well.

User avatar
viacin
Active Member
Posts: 344
Joined: September 30th, 2008, 6:25 pm
Location: Alabama, USA

Post by viacin » October 19th, 2008, 8:43 pm

lol, gotta watch those fumes bud...

maybe no one has any for sale at the moment. I still see HCl and sulfuric acid for auction, although for almost twice the price you pay at the hardware store.
Of all the contrivances for cheating the laboring classes of mankind, none has been more effective than that which deludes them with paper money. - Daniel Webster

bmgold
Active Member
Posts: 183
Joined: September 28th, 2008, 10:46 am
Location: Pennsylvania

ebay nitric

Post by bmgold » October 21st, 2008, 5:54 am

I found the link again on nitric acid on ebay. It has ended but WAS on there. I didn't make it up afterall.

260268502825

Username : dudadiesel

Keep watching this user or maybe send him a message to get another batch listed. Maybe he is just out now or didn't get any responses or maybe he will list more soon

Just a thought

User avatar
viacin
Active Member
Posts: 344
Joined: September 30th, 2008, 6:25 pm
Location: Alabama, USA

Post by viacin » October 21st, 2008, 6:37 pm

hey, thanks for finding it. That's the same guy that sells sulfuric acid too. 1 gallon for $56 is cheaper than anything I've seen, but still not as cheap as making it yourself.

He says "does not ship with bases", like sodium nitrate. But I wonder if he has thought about shipping it with his sulfuric acid. If it spilled out and mixed with the cardboard box he would have a big 'ol batch of guncotton :p
Of all the contrivances for cheating the laboring classes of mankind, none has been more effective than that which deludes them with paper money. - Daniel Webster

User avatar
DarkspARCS
Active Member
Posts: 318
Joined: December 11th, 2010, 4:13 am
Country of Origin: U.S.A.
Location: U.S.A.

Re: home made cupels

Post by DarkspARCS » June 9th, 2013, 8:46 pm

ok... fine. I'll be the first n00b to post here. Laser Steve, is the offer of free cupels to the first 5 n00bs who post here still good? :P :twisted:

We're almost out and we have so much ore testing left to do lol... :roll:
Thanks for your time

- Richard

"Earth has only one absolute, which is centrifugal force. Anything is possible when you put a spin to it...."

AndyWilliams
Active Member
Posts: 369
Joined: July 7th, 2012, 11:43 pm
Country of Origin: US
Location: Green Bay, Wi

Re:

Post by AndyWilliams » June 9th, 2013, 9:27 pm

Harold_V wrote:
JOE S (INDY) wrote:'The Crotchity Old
I resent you stealing my title! :lol:

Harold
Nonsense! You're the crochEty one, kind of like the difference between Sodium Metabisulfite, and Sodium Metabisulfate!

Pogo
Member
Posts: 2
Joined: September 30th, 2013, 6:06 pm
Country of Origin: America

Re: home made cupels

Post by Pogo » September 30th, 2013, 7:36 pm

Hello,
This comes from my book; Fire Assay, by Orson Cutler Shephard and Waldemar F. Dietrich Copy right 1940: Portland cement alone is sometimes used for assay cupels; it is more commonly used with various percentages of bone ash. When cement is used as all or part of the cupel composition the amount of mixing water should be 8 to 12 per cent. Less or more cause the cement to check or crack on heating. Pure cement cupels give higher cupellation loss than do bone ash cupels, but mixtures of cement and bone ash up to 75% cement give as low a percentage of losses as those made of pure bone ash. Have fun!

P.S. It took me two years to puzzle out how to perform a fire assay. I found this book in a Colorado used book store about four years after (I thought), mastering the process. This book has helped greatly, is probably one of the books you'll never find in the library, and goes into fire assay with such scope and depth that I feel overwhelmed.