Can you do some gravity test . ? How heavy is it . Measurements density .View attachment 51460View attachment 51461View attachment 51462View attachment 51463View attachment 51464View attachment 51465View attachment 51466View attachment 51467View attachment 51468View attachment 51469View attachment 51470View attachment 51471View attachment 51472View attachment 51473View attachment 51474View attachment 51475View attachment 51476View attachment 51477View attachment 51478View attachment 51479View attachment 51480View attachment 51481View attachment 51482View attachment 51483View attachment 51484View attachment 51485View attachment 51486View attachment 51487View attachment 51488
Yes I was thinking about it. Later in my zone. I need to find appropriate container to do it with, because they are larger than usual. I've done alot of smaller gravity testing, I can say they have PGM weight. Later I will work on that, please check back...Can you do some gravity test . ? How heavy is it . Measurements density .
Nuggets. Other members are .processing some now. Not polished, tarnish removed yes. PGMs have iron, chromite, etc. So, they get placed in water/hydrochloric acid for a bath. The reason large sizes is because the faults are quite big.Nuggets ? Or polished sulfidic ore rocks ?
But then you sayI need to find appropriate container to do it with, because they are larger than usual. I've done alot of smaller gravity testing,
So you have a container big enough to soak them in water/HCl - but not big enough to do a specific gravity test in ???they get placed in water/hydrochloric acid for a bath.
Lead is heavy to - being heavy doesn't make it silver gold or PGMsI can say they have PGM weight
Well Lead is 11.3, Silver 10.5, Rh 12.4, Pd 12.1 and the Pt at 22 and IR OS and such at 24.But then you say
So you have a container big enough to soak them in water/HCl - but not big enough to do a specific gravity test in ???
Lead is heavy to - being heavy doesn't make it silver gold or PGMs
Kurt
Per the bold print - & that is my pointWell Lead is 11.3, Silver 10.5, Rh 12.4, Pd 12.1 and the Pt at 22 and IR OS and such at 24.
But that is pure metal, ore is a whole other realm.